Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.141 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHPd |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 0.000 | 154.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 0.000 | 218.1 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 0.003 | 137.1 |
Si (mp-149) | <1 1 1> | <1 1 1> | 0.004 | 207.8 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 0.004 | 154.2 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 0.005 | 218.1 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 0.006 | 207.8 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 0.012 | 154.2 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 0.013 | 218.1 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 0.013 | 72.7 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 0.014 | 154.2 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 0.014 | 218.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 0.015 | 290.9 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 0.015 | 154.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 0.015 | 291.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 0.016 | 154.2 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 0.016 | 218.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 0.017 | 274.2 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 0.017 | 222.8 |
C (mp-66) | <1 1 0> | <1 1 0> | 0.019 | 72.7 |
C (mp-66) | <1 1 1> | <1 1 1> | 0.019 | 89.1 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 0.020 | 137.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 0.020 | 85.7 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 0.027 | 89.1 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 0.027 | 274.2 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 0.028 | 218.1 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 0.032 | 154.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 0.034 | 89.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 0.034 | 169.7 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 0.034 | 218.1 |
C (mp-48) | <1 1 1> | <1 1 0> | 0.041 | 169.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 0.041 | 154.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 0.043 | 218.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 0.043 | 169.7 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 0.043 | 308.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 0.044 | 218.1 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 0> | 0.047 | 205.7 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 0.049 | 266.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 0.050 | 17.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 0.051 | 85.7 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 0.052 | 257.1 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 0.053 | 257.1 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 0.053 | 24.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 0.054 | 29.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 0.055 | 218.1 |
C (mp-48) | <0 0 1> | <1 1 1> | 0.060 | 207.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 0.062 | 118.7 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 0.064 | 207.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 0.064 | 85.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 0.076 | 274.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
200 | 161 | 161 | 0 | 0 | 0 |
161 | 200 | 161 | 0 | 0 | 0 |
161 | 161 | 200 | 0 | 0 | 0 |
0 | 0 | 0 | 60 | 0 | 0 |
0 | 0 | 0 | 0 | 60 | 0 |
0 | 0 | 0 | 0 | 0 | 60 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
17.7 | -7.9 | -7.9 | 0 | 0 | 0 |
-7.9 | 17.7 | -7.9 | 0 | 0 | 0 |
-7.9 | -7.9 | 17.7 | 0 | 0 | 0 |
0 | 0 | 0 | 16.6 | 0 | 0 |
0 | 0 | 0 | 0 | 16.6 | 0 |
0 | 0 | 0 | 0 | 0 | 16.6 |
Shear Modulus GV44 GPa |
Bulk Modulus KV174 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR174 GPa |
Shear Modulus GVRH38 GPa |
Bulk Modulus KVRH174 GPa |
Elastic Anisotropy1.71 |
Poisson's Ratio0.40 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.039 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
TiH (mp-1060435) | 0.0000 | 0.044 | 2 |
USe (mp-911057) | 0.0000 | 0.146 | 2 |
TcC (mp-1009876) | 0.0000 | 0.650 | 2 |
TcC (mp-1009837) | 0.0000 | 0.650 | 2 |
MgCd (mp-1039157) | 0.0000 | 0.249 | 2 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.393 | 1 |
C (mp-998866) | 0.0000 | 2.763 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Na (mp-1093989) | 0.0000 | 1.074 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Pd |
Final Energy/Atom-4.3492 eV |
Corrected Energy-8.6984 eV
-8.6984 eV = -8.6984 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)