Final Magnetic Moment3.118 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.173 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 216.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 288.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 216.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 216.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 204.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 255.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 216.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 216.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 288.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 255.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 88.5 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 255.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 216.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 216.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 72.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 88.5 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 88.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 306.4 |
Al (mp-134) | <1 1 1> | <1 0 0> | 255.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 255.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 255.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 288.9 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 216.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 72.2 |
C (mp-66) | <1 1 1> | <1 1 1> | 88.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 288.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 255.3 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 306.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 153.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 255.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 144.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 204.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 265.4 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 216.7 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 265.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 255.3 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 255.3 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 255.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 88.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 216.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 288.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 255.3 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 265.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 255.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 144.4 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 204.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 255.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 153.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 144.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 72.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
140 | 55 | 55 | -3 | -3 | 3 |
55 | 140 | 55 | -3 | -3 | 3 |
55 | 55 | 140 | -3 | -3 | 3 |
-3 | -3 | -3 | 55 | 0 | 0 |
-3 | -3 | -3 | 0 | 55 | 0 |
3 | 3 | 3 | 0 | 0 | 55 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.2 | -2.6 | -2.6 | 0.2 | 0.3 | -0.3 |
-2.6 | 9.2 | -2.6 | 0.3 | 0.2 | -0.3 |
-2.6 | -2.6 | 9.2 | 0.3 | 0.3 | -0.2 |
0.2 | 0.3 | 0.3 | 18.1 | 0 | 0 |
0.3 | 0.2 | 0.3 | 0 | 18.1 | 0 |
-0.3 | -0.3 | -0.2 | 0 | 0 | 18.1 |
Shear Modulus GV50 GPa |
Bulk Modulus KV84 GPa |
Shear Modulus GR49 GPa |
Bulk Modulus KR83 GPa |
Shear Modulus GVRH50 GPa |
Bulk Modulus KVRH83 GPa |
Elastic Anisotropy0.10 |
Poisson's Ratio0.25 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
YbCo2 (mp-281) | 0.0000 | 0.048 | 2 |
UIr2 (mp-1655) | 0.0000 | 0.045 | 2 |
SmAl2 (mp-2358) | 0.0000 | 0.000 | 2 |
YIr2 (mp-2762) | 0.0000 | 0.000 | 2 |
DyFe2 (mp-1757) | 0.0000 | 0.147 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Fe_pv |
Final Energy/Atom-7.3257 eV |
Corrected Energy-43.9543 eV
-43.9543 eV = -43.9543 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)