Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.603 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaH2 |
Band Gap0.856 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 101.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 70.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 239.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 122.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 101.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 81.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 203.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 142.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 50.4 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 262.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 311.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 163.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 201.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 37.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 101.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 239.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 61.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 203.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 143.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 325.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 325.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 163.0 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 287.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 61.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 201.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 61.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 211.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 105.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 183.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 215.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 311.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 163.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 201.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 262.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 183.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 163.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 262.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 183.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 88.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 113.4 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 119.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 224.1 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 262.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 183.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 203.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 163.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 282.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 142.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaHgPb (mp-20879) | 0.3607 | 0.076 | 3 |
YbHgPb (mp-571493) | 0.2176 | 0.080 | 3 |
SmTlCd (mp-1019255) | 0.3902 | 0.002 | 3 |
CeTlCd (mp-1018668) | 0.0698 | 0.045 | 3 |
CeInCu (mp-1077348) | 0.3252 | 0.133 | 3 |
BaF2 (mp-8644) | 0.0201 | 0.136 | 2 |
YHg2 (mp-30725) | 0.0277 | 0.015 | 2 |
Sr2Si (mp-13051) | 0.0228 | 0.078 | 2 |
Rb2S (mp-1071288) | 0.0227 | 0.088 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv H |
Final Energy/Atom-3.4291 eV |
Corrected Energy-20.5748 eV
-20.5748 eV = -20.5748 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)