material

DyCoO3

ID:

mp-22137


Tags: Dysprosium cobaltate(III) Dysprosium cobalt oxide Perovskite Dysprosium cobalt(III) oxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.662 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.006 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Co3O4 + CoO2 + Dy2O3
Band Gap
1.183 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 23658 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.011 230.4
WS2 (mp-224) <1 0 1> <1 1 1> 0.011 324.0
SiC (mp-7631) <1 0 1> <0 0 1> 0.015 237.5
LiGaO2 (mp-5854) <1 1 0> <0 1 0> 0.015 193.5
LiNbO3 (mp-3731) <1 1 1> <1 0 1> 0.016 259.8
GaSe (mp-1943) <1 0 1> <1 0 1> 0.024 207.9
TiO2 (mp-390) <1 0 1> <0 0 1> 0.026 118.8
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.031 326.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.036 172.8
YAlO3 (mp-3792) <0 1 0> <0 1 0> 0.041 38.7
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.047 155.9
LiNbO3 (mp-3731) <1 0 0> <0 1 1> 0.051 146.3
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.053 89.1
WS2 (mp-224) <0 0 1> <1 1 1> 0.058 194.4
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.058 194.4
KCl (mp-23193) <1 1 0> <0 1 0> 0.060 116.1
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.063 154.8
TiO2 (mp-390) <1 1 1> <0 1 0> 0.066 270.9
ZnO (mp-2133) <1 1 1> <1 0 0> 0.068 128.0
C (mp-48) <1 0 0> <1 1 0> 0.077 57.6
MgO (mp-1265) <1 1 0> <0 1 0> 0.078 77.4
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.079 230.4
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.079 194.4
BN (mp-984) <1 0 0> <1 1 0> 0.079 57.6
Mg (mp-153) <0 0 1> <1 1 1> 0.080 194.4
ZrO2 (mp-2858) <0 1 1> <0 1 1> 0.083 195.1
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.084 193.5
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.089 255.9
LiTaO3 (mp-3666) <1 0 0> <0 1 1> 0.095 146.3
CdS (mp-672) <1 0 1> <1 1 0> 0.101 230.4
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.103 348.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.105 128.0
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.106 348.3
MgO (mp-1265) <1 1 1> <0 1 0> 0.113 154.8
LaF3 (mp-905) <1 0 0> <1 0 0> 0.118 213.3
C (mp-48) <1 1 0> <1 1 0> 0.122 230.4
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.122 128.0
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.127 172.8
C (mp-48) <1 0 1> <1 0 0> 0.130 255.9
GaSe (mp-1943) <0 0 1> <1 0 0> 0.133 298.6
PbS (mp-21276) <1 1 0> <0 1 0> 0.134 154.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.141 148.4
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.143 267.2
GaP (mp-2490) <1 1 0> <1 1 0> 0.145 172.8
LiNbO3 (mp-3731) <1 0 1> <1 1 0> 0.145 230.4
LiTaO3 (mp-3666) <1 1 1> <1 0 1> 0.146 259.8
Mg (mp-153) <1 1 0> <0 1 0> 0.146 116.1
Ni (mp-23) <1 1 0> <0 1 0> 0.153 154.8
AlN (mp-661) <1 1 0> <1 0 0> 0.154 298.6
GaN (mp-804) <1 0 0> <0 1 0> 0.161 116.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TmCoO3 (mp-686908) 0.1318 0.022 3
TmNiO3 (mp-19002) 0.1114 0.006 3
LuCoO3 (mp-561616) 0.1510 0.026 3
ErNiO3 (mp-18983) 0.1511 0.000 3
HoCoO3 (mp-24875) 0.1008 0.016 3
HoMg(NiO3)2 (mvc-10217) 0.3468 0.080 4
HoMg(CoO3)2 (mvc-10209) 0.3314 0.140 4
CaHo(CoO3)2 (mvc-10306) 0.3265 0.079 4
LiSm2IrO6 (mp-11904) 0.3468 0.000 4
LiSm2OsO6 (mp-12448) 0.3545 0.000 4
Mn3O4 (mp-25696) 0.6462 0.053 2
Fe3O4 (mp-715275) 0.7175 0.748 2
Al2O3 (mp-642363) 0.6809 0.280 2
Cr3C2 (mp-570112) 0.7067 0.030 2
Mn3O4 (mp-715570) 0.6573 0.053 2
CaLaMnSnO6 (mp-694915) 0.4246 0.117 5
CaDyMnSnO6 (mp-706325) 0.3605 0.211 5
CaSmMnSnO6 (mp-698702) 0.3252 0.176 5
CaLaFeAgO6 (mvc-8977) 0.3837 0.054 5
CaLaCrSbO6 (mvc-9973) 0.4128 0.203 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Dy_3 Co O
Final Energy/Atom
-7.1775 eV
Corrected Energy
-159.4741 eV
-159.4741 eV = -143.5506 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 190951
  • 190949
  • 172047
  • 190950
  • 23658
Submitted by
User remarks:
  • Dysprosium cobaltate(III)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)