Final Magnetic Moment0.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.112 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 225.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 207.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 225.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 173.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 126.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 296.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 292.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 207.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 147.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 272.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 61.9 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 219.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 225.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 292.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 61.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 198.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.0 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 193.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 111.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 61.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 309.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 272.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 86.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 260.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 251.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 210.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 225.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 161.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 353.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 161.0 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 160.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 148.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 222.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 268.1 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 268.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 86.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 111.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 173.4 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 207.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 89.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 193.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 207.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 321.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 251.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 49.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 222.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 198.2 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 237.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
230 | 156 | 19 | 0 | 0 | 0 |
156 | 230 | 19 | 0 | 0 | 0 |
19 | 19 | 578 | 0 | 0 | 0 |
0 | 0 | 0 | 30 | 0 | 0 |
0 | 0 | 0 | 0 | 30 | 0 |
0 | 0 | 0 | 0 | 0 | 131 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8 | -5.4 | -0.1 | 0 | 0 | 0 |
-5.4 | 8 | -0.1 | 0 | 0 | 0 |
-0.1 | -0.1 | 1.7 | 0 | 0 | 0 |
0 | 0 | 0 | 33.3 | 0 | 0 |
0 | 0 | 0 | 0 | 33.3 | 0 |
0 | 0 | 0 | 0 | 0 | 7.7 |
Shear Modulus GV94 GPa |
Bulk Modulus KV159 GPa |
Shear Modulus GR47 GPa |
Bulk Modulus KR152 GPa |
Shear Modulus GVRH71 GPa |
Bulk Modulus KVRH155 GPa |
Elastic Anisotropy5.00 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaHN (mp-34932) | 0.3035 | 0.000 | 3 |
BaSiC (mp-1009828) | 0.5934 | 0.874 | 3 |
LuC2 (mp-8371) | 0.1558 | 0.108 | 2 |
PaC2 (mp-1018130) | 0.0613 | 0.033 | 2 |
CaN2 (mp-1009657) | 0.1273 | 0.000 | 2 |
TmC2 (mp-269) | 0.1737 | 0.085 | 2 |
CeC2 (mp-2839) | 0.1802 | 0.053 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U C |
Final Energy/Atom-10.0274 eV |
Corrected Energy-30.0821 eV
-30.0821 eV = -30.0821 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)