Final Magnetic Moment0.284 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.083 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.451 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3(AsO4)2 + CoO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 254.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 238.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 254.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 254.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 305.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 152.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 254.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 238.7 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 197.3 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 119.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 152.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 190.6 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 254.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 203.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 305.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 305.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 101.7 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 216.0 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 238.7 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 254.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 216.0 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 101.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 108.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 50.8 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 190.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 254.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 152.5 |
C (mp-66) | <1 0 0> | <1 1 0> | 190.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 203.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 254.2 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 238.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 203.3 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 108.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 50.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 254.2 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 108.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 203.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 101.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 50.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 254.2 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 254.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 1> | 238.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 203.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 254.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 305.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 50.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 254.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 101.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 203.3 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 119.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe8SiO12 (mp-763415) | 0.3475 | 0.062 | 3 |
Zn2SiO4 (mp-1020717) | 0.3887 | 0.122 | 3 |
Co2SiO4 (mp-18941) | 0.3606 | 0.046 | 3 |
Mg2SiO4 (mp-5391) | 0.3272 | 0.050 | 3 |
Mn2GeO4 (mp-25702) | 0.2919 | 1.394 | 3 |
LiCo2OF3 (mp-763919) | 0.4173 | 0.263 | 4 |
LiNi2OF3 (mp-766749) | 0.4122 | 0.103 | 4 |
LiFe2OF3 (mp-851047) | 0.4086 | 0.512 | 4 |
LiMn2OF3 (mp-763454) | 0.4178 | 0.072 | 4 |
Mn7SbAsO12 (mp-699691) | 0.1635 | 0.000 | 4 |
Mn9Zn6Si4(SbO14)2 (mp-850230) | 0.5669 | 0.000 | 5 |
Mn13Al4Si2(SbO14)2 (mp-565677) | 0.6170 | 0.000 | 5 |
Al4Co13Si2(SbO14)2 (mvc-9355) | 0.6097 | 0.019 | 5 |
Al4Si2Ni13(SbO14)2 (mvc-9362) | 0.6267 | 0.014 | 5 |
Al4Fe13Si2(SbO14)2 (mvc-9528) | 0.6058 | 0.208 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co As O |
Final Energy/Atom-5.6981 eV |
Corrected Energy-282.4099 eV
-282.4099 eV = -239.3190 eV (uncorrected energy) - 26.2360 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)