material

HfAl

ID:

mp-249

DOI:

10.17188/1200313


Tags: Aluminium hafnium (1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.396 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.013 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Hf4Al3 + HfAl2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 107828 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.011 293.5
ZrO2 (mp-2858) <0 1 1> <1 1 0> 0.023 195.4
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.026 140.4
Cu (mp-30) <1 0 0> <1 0 1> 0.036 117.4
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.048 209.8
BN (mp-984) <1 0 0> <0 1 0> 0.060 153.8
SiC (mp-8062) <1 1 1> <1 0 1> 0.075 234.8
C (mp-48) <1 0 0> <0 1 0> 0.078 209.8
SiO2 (mp-6930) <0 0 1> <1 1 0> 0.116 195.4
DyScO3 (mp-31120) <0 1 1> <0 0 1> 0.118 106.2
C (mp-66) <1 0 0> <0 1 0> 0.124 167.8
C (mp-48) <1 0 1> <0 0 1> 0.129 318.7
Ge (mp-32) <1 0 0> <0 1 0> 0.130 167.8
CdWO4 (mp-19387) <0 0 1> <0 1 0> 0.138 181.8
Fe2O3 (mp-24972) <0 0 1> <0 1 0> 0.138 251.8
SiO2 (mp-6930) <1 1 1> <0 1 1> 0.151 266.5
TiO2 (mp-390) <0 0 1> <1 0 1> 0.154 58.7
CdS (mp-672) <1 1 0> <0 1 0> 0.168 251.8
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.177 321.7
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.178 212.5
TiO2 (mp-390) <1 1 0> <0 0 1> 0.178 106.2
C (mp-48) <0 0 1> <0 1 0> 0.180 42.0
Ni (mp-23) <1 1 0> <0 1 1> 0.181 190.4
KTaO3 (mp-3614) <1 1 0> <0 1 1> 0.184 114.2
GdScO3 (mp-5690) <1 0 1> <0 1 1> 0.188 114.2
BN (mp-984) <0 0 1> <0 1 0> 0.188 97.9
AlN (mp-661) <0 0 1> <0 1 0> 0.191 153.8
TePb (mp-19717) <1 0 0> <0 0 1> 0.191 212.5
PbS (mp-21276) <1 1 1> <1 0 0> 0.194 187.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.194 177.0
MgAl2O4 (mp-3536) <1 1 0> <0 1 1> 0.195 190.4
Cu (mp-30) <1 1 1> <0 1 0> 0.220 251.8
GaAs (mp-2534) <1 0 0> <0 1 0> 0.222 167.8
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.227 212.5
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.229 106.2
LaAlO3 (mp-2920) <0 0 1> <0 1 0> 0.233 153.8
Al2O3 (mp-1143) <1 0 1> <0 1 0> 0.240 335.7
C (mp-66) <1 1 0> <0 1 0> 0.241 195.8
Al (mp-134) <1 1 0> <0 1 1> 0.243 114.2
SiC (mp-7631) <1 0 0> <1 0 1> 0.248 234.8
SiC (mp-11714) <1 0 1> <0 1 0> 0.254 223.8
Au (mp-81) <1 1 1> <0 1 0> 0.259 335.7
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.261 106.2
Ge (mp-32) <1 1 0> <0 1 1> 0.281 190.4
ZnSe (mp-1190) <1 0 0> <0 1 0> 0.293 167.8
GaN (mp-804) <1 0 1> <0 1 1> 0.302 38.1
CdWO4 (mp-19387) <1 1 1> <0 1 0> 0.316 209.8
ZnO (mp-2133) <1 1 0> <0 1 0> 0.318 153.8
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.326 58.7
InAs (mp-20305) <1 1 1> <1 1 0> 0.330 195.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
207 55 97 0 0 0
55 228 67 0 0 0
97 67 182 0 0 0
0 0 0 68 0 0
0 0 0 0 122 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
6.5 -0.6 -3.2 0 0 0
-0.6 5 -1.5 0 0 0
-3.2 -1.5 7.8 0 0 0
0 0 0 14.7 0 0
0 0 0 0 8.2 0
0 0 0 0 0 14.8
Shear Modulus GV
78 GPa
Bulk Modulus KV
117 GPa
Shear Modulus GR
71 GPa
Bulk Modulus KR
117 GPa
Shear Modulus GVRH
74 GPa
Bulk Modulus KVRH
117 GPa
Elastic Anisotropy
0.51
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZrAl (mp-11233) 0.2045 0.023 2
ThAu (mp-1018175) 0.5784 0.000 2
MgSi (mp-1073737) 0.3866 0.234 2
ZrCu (mp-1067210) 0.4801 0.024 2
CaMg (mp-1039350) 0.5910 0.025 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Al
Final Energy/Atom
-7.2469 eV
Corrected Energy
-28.9876 eV
-28.9876 eV = -28.9876 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 107828
  • 608084
  • 608086
Submitted by
User remarks:
  • Aluminium hafnium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)