Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr2FeClO3 + SrCl2 + Fe2O3 |
Band Gap1.084 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 288.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 224.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 320.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 368.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 144.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 137.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 288.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 80.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 80.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 176.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 320.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 240.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 336.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 256.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 336.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 352.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 80.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 336.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 128.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 137.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 160.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 64.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 80.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 32.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 137.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 288.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 112.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 138.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 320.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 256.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 208.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 160.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 144.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 240.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 240.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 208.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 208.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 288.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 144.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 272.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 240.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 240.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 256.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 176.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 96.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr3Co2Cl2O5 (mp-561603) | 0.1748 | 0.137 | 4 |
Ca3Fe2Cl2O5 (mp-566329) | 0.2356 | 0.030 | 4 |
Ba3In2Cl2O5 (mp-559933) | 0.3463 | 0.005 | 4 |
Ba3In2Br2O5 (mp-556004) | 0.1217 | 0.008 | 4 |
Sr3Co2Cl2O5 (mp-24846) | 0.2445 | 0.137 | 4 |
Sr3Fe2Cu2Se2O5 (mp-565357) | 0.6516 | 0.000 | 5 |
Sr3Fe2Cu2S2O5 (mvc-3218) | 0.6589 | 0.036 | 5 |
Sr3Cr2Cu2S2O5 (mvc-13306) | 0.6538 | 0.077 | 5 |
Sr3Sc2Cu2S2O5 (mp-15900) | 0.6909 | 0.041 | 5 |
Sr3Fe2Cu2S2O5 (mp-505310) | 0.6535 | 0.036 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: O Cl Fe_pv Sr_sv |
Final Energy/Atom-5.9519 eV |
Corrected Energy-80.3999 eV
-80.3999 eV = -71.4225 eV (uncorrected energy) - 5.4660 eV (MP Advanced Correction) - 3.5114 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)