Material Details

Final Magnetic Moment
20.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-2.917 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.99 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.649 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-48) <1 1 0> <1 0 0> 0.000 133.4
BN (mp-984) <1 1 1> <0 1 0> 0.001 169.7
TiO2 (mp-390) <0 0 1> <1 0 1> 0.006 216.7
AlN (mp-661) <1 0 1> <1 0 0> 0.007 88.9
LaF3 (mp-905) <1 0 1> <0 1 1> 0.012 210.1
Ga2O3 (mp-886) <1 0 -1> <1 1 0> 0.012 307.3
NdGaO3 (mp-3196) <1 1 0> <1 1 0> 0.021 61.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.021 216.7
Ni (mp-23) <1 0 0> <1 1 0> 0.022 61.5
LiAlO2 (mp-3427) <0 0 1> <1 1 0> 0.022 245.8
MgO (mp-1265) <1 0 0> <1 1 0> 0.024 307.3
YVO4 (mp-19133) <1 0 1> <0 1 1> 0.026 210.1
ZnTe (mp-2176) <1 0 0> <1 1 0> 0.034 307.3
CaF2 (mp-2741) <1 1 1> <0 1 0> 0.037 212.1
CdSe (mp-2691) <1 0 0> <1 1 0> 0.037 307.3
CsI (mp-614603) <1 0 0> <1 1 0> 0.038 61.5
InAs (mp-20305) <1 0 0> <1 1 0> 0.042 307.3
NdGaO3 (mp-3196) <0 1 0> <0 1 0> 0.043 42.4
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.043 137.6
NdGaO3 (mp-3196) <0 1 1> <0 1 1> 0.044 52.5
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.045 278.7
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.050 92.9
C (mp-48) <0 0 1> <0 0 1> 0.051 185.8
LiGaO2 (mp-5854) <1 0 0> <0 1 1> 0.052 105.1
BN (mp-984) <0 0 1> <0 0 1> 0.052 247.7
NdGaO3 (mp-3196) <1 1 1> <1 1 1> 0.053 68.8
GaSb (mp-1156) <1 0 0> <1 1 0> 0.054 307.3
SrTiO3 (mp-4651) <1 1 1> <0 1 1> 0.058 210.1
ZrO2 (mp-2858) <0 1 1> <1 1 1> 0.063 275.3
TiO2 (mp-2657) <1 1 0> <0 1 1> 0.064 157.6
ZrO2 (mp-2858) <0 0 1> <1 1 0> 0.066 245.8
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.066 216.7
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.067 84.9
TeO2 (mp-2125) <1 0 1> <0 0 1> 0.068 154.8
Al (mp-134) <1 1 0> <0 0 1> 0.071 92.9
GaAs (mp-2534) <1 1 0> <0 0 1> 0.072 92.9
Si (mp-149) <1 1 0> <0 1 0> 0.073 42.4
CeO2 (mp-20194) <1 1 0> <0 1 0> 0.075 42.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.077 92.9
GaP (mp-2490) <1 1 1> <0 1 0> 0.079 212.1
Mg (mp-153) <1 1 1> <0 1 1> 0.080 210.1
PbSe (mp-2201) <1 0 0> <1 1 0> 0.084 307.3
TiO2 (mp-390) <1 1 0> <0 1 1> 0.086 52.5
CaF2 (mp-2741) <1 0 0> <1 1 0> 0.093 61.5
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.094 247.7
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.105 133.4
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.105 133.4
C (mp-48) <1 0 0> <1 0 0> 0.110 133.4
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.123 31.0
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.123 92.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
262 123 129 0 0 0
123 260 116 0 0 0
129 116 277 0 0 0
0 0 0 83 0 0
0 0 0 0 76 0
0 0 0 0 0 104
Compliance Tensor Sij (10-12Pa-1)
5.6 -1.8 -1.8 0 0 0
-1.8 5.3 -1.4 0 0 0
-1.8 -1.4 5 0 0 0
0 0 0 12 0 0
0 0 0 0 13.2 0
0 0 0 0 0 9.6
Shear Modulus GV
82 GPa
Bulk Modulus KV
170 GPa
Shear Modulus GR
80 GPa
Bulk Modulus KR
170 GPa
Shear Modulus GVRH
81 GPa
Bulk Modulus KVRH
170 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca2FeIrO6 (mvc-5784) 0.1506 0.000 4
CaHoCr2O6 (mvc-10297) 0.1299 0.032 4
Ca2NiOsO6 (mp-510537) 0.1499 0.000 4
Sm2MgIrO6 (mp-980108) 0.1213 0.006 4
Tb2MnNiO6 (mp-645135) 0.1486 0.000 4
Pb3O4 (mp-636813) 0.6421 0.037 2
Mn5O8 (mp-18922) 0.6030 0.029 2
Mn5O8 (mp-715008) 0.6094 0.029 2
Pb2O3 (mp-20078) 0.6367 0.010 2
Cr5S8 (mp-849084) 0.6788 0.000 2
YTiO3 (mvc-14477) 0.1145 0.060 3
CeCrO3 (mp-780921) 0.1038 0.057 3
GdGaO3 (mp-18656) 0.1077 0.049 3
DyGaO3 (mp-755612) 0.0884 0.048 3
TbGaO3 (mp-756290) 0.0632 0.047 3
CaLaFeMoO6 (mvc-9015) 0.2140 0.010 5
CaLaFeAgO6 (mvc-8977) 0.1535 0.056 5
CaLaCrSbO6 (mvc-9973) 0.1586 0.086 5
CaLaMnMoO6 (mp-705412) 0.1927 0.000 5
CaLaMnRuO6 (mp-690556) 0.1615 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: O Fe_pv Sm_3
Final Energy/Atom
-7.5460 eV
Corrected Energy
-170.2792 eV
-170.2792 eV = -150.9197 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 252078
  • 291099
  • 252077
  • 252076
  • 161780
  • 189727
  • 82424
  • 93606
  • 27276
Submitted by
User remarks:
  • Samarium ferrate(III)
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)