Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.462 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoCl6 + MoO2 |
Band Gap2.459 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiC (mp-7631) | <0 0 1> | <0 0 1> | 266.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 266.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 272.2 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 267.8 |
C (mp-48) | <1 0 0> | <1 0 0> | 267.8 |
C (mp-48) | <1 1 1> | <0 1 0> | 272.2 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 272.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 311.1 |
SrTiO3 (mp-4651) | <1 1 0> | <0 1 0> | 311.1 |
CsI (mp-614603) | <1 0 0> | <0 1 0> | 311.1 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 350.0 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 0> | 350.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 128.4 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 311.1 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 194.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 267.8 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 267.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 256.9 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 267.8 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 194.4 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 194.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 272.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 233.3 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 267.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 116.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 272.2 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 267.8 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 89.3 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 350.0 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 272.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 311.1 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 267.8 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 272.2 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 267.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 116.7 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 267.8 |
CaF2 (mp-2741) | <1 1 0> | <0 1 0> | 350.0 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 155.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 272.2 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 155.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 267.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 267.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 194.4 |
C (mp-48) | <0 0 1> | <0 1 0> | 272.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 155.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 267.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 233.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 89.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 194.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 155.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VOF3 (mp-764274) | 0.4861 | 0.011 | 3 |
VOF3 (mp-765770) | 0.5877 | 0.022 | 3 |
ReCl3O2 (mp-607436) | 0.6105 | 0.000 | 3 |
VOF3 (mp-565784) | 0.5996 | 0.000 | 3 |
LiH2N (mp-1087524) | 0.6145 | 0.098 | 3 |
KCa(H2N)3 (mp-720856) | 0.5968 | 0.000 | 4 |
MoSeCl7O (mp-573045) | 0.6859 | 0.011 | 4 |
TeMoCl7O (mp-617022) | 0.7090 | 0.015 | 4 |
TlMo2Cl7O2 (mp-566031) | 0.6409 | 0.021 | 4 |
RbCa(H2N)3 (mp-696329) | 0.6638 | 0.000 | 4 |
VF4 (mp-765926) | 0.7301 | 0.058 | 2 |
ZrCl4 (mp-569175) | 0.7379 | 0.000 | 2 |
SCl2 (mp-28128) | 0.6236 | 0.062 | 2 |
NaH4CNO2 (mp-706281) | 0.7467 | 0.161 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv Cl O |
Final Energy/Atom-4.5263 eV |
Corrected Energy-107.4594 eV
-107.4594 eV = -90.5262 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)