Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.539 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.911 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nbm [125] |
HallP 4 2 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 160.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 266.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 213.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 320.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 320.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 213.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 266.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 151.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 320.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 222.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 266.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 222.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 213.5 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 151.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 266.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 160.2 |
BN (mp-984) | <1 1 1> | <1 1 0> | 302.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 213.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 320.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 226.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 160.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 213.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 222.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 266.9 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 226.5 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 246.9 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 160.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 213.5 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 123.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 320.3 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 111.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 160.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 266.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 53.4 |
C (mp-66) | <1 1 1> | <1 1 0> | 226.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 266.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 222.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 222.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 111.3 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 226.5 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 151.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 151.0 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 213.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 111.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 53.4 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 222.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 213.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 302.0 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 320.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaMoN3 (mp-989631) | 0.7154 | 0.000 | 3 |
SrTcN3 (mp-989627) | 0.6173 | 0.000 | 3 |
LaCrN3 (mp-989612) | 0.7260 | 0.000 | 3 |
Na2Ca(AsO3)4 (mp-560545) | 0.4097 | 0.018 | 4 |
Li2Fe(PO3)4 (mp-762651) | 0.4009 | 0.171 | 4 |
SrV4(AgO6)2 (mp-566224) | 0.2006 | 0.000 | 4 |
CaV4(AgO6)2 (mp-25168) | 0.0870 | 0.000 | 4 |
Na2SrV4O12 (mp-18975) | 0.1545 | 0.000 | 4 |
Nd3Al3Si3(NO6)2 (mp-695170) | 0.6788 | 0.006 | 5 |
CaScAlSiO6 (mp-39167) | 0.7156 | 0.000 | 5 |
CaAl2Si(HO2)4 (mp-643941) | 0.6199 | 0.017 | 5 |
Zn3TeAs2Pb3O14 (mp-558298) | 0.6922 | 0.000 | 5 |
Sr3TaGa3(SiO7)2 (mp-16136) | 0.7040 | 0.000 | 5 |
Na2Ca6Mg7Fe(SiO3)16 (mp-745155) | 0.7416 | 0.031 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv Ca_sv V_pv O |
Final Energy/Atom-7.0215 eV |
Corrected Energy-296.9067 eV
Uncorrected energy = -266.8187 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.700 eV/atom x 8.0 atoms) = -13.6000 eV
Corrected energy = -296.9067 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)