Final Magnetic Moment0.035 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.538 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCuO2 + Li3CuO3 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 313.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 252.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 90.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 183.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 264.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 306.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 234.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 234.7 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 124.8 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 270.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 264.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 245.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 306.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 264.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 214.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 168.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 330.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 234.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 234.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 330.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 245.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 61.2 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 234.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 252.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 245.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 264.5 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 234.7 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 234.7 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 252.7 |
MoS2 (mp-1434) | <1 0 1> | <1 1 0> | 270.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 183.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 252.7 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 313.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 330.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 183.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 330.6 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 330.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 306.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 264.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 264.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 245.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 306.2 |
BN (mp-984) | <1 1 1> | <1 0 0> | 245.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 252.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 252.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 234.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 306.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 313.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 61.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 252.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCoO2 (mvc-14630) | 0.5504 | 0.441 | 3 |
ZnNiO2 (mvc-15568) | 0.5470 | 0.389 | 3 |
CaNiO2 (mvc-13785) | 0.5409 | 0.451 | 3 |
Li4(CuO2)3 (mp-758475) | 0.3631 | 0.009 | 3 |
Li3MnO3 (mp-769747) | 0.4830 | 0.265 | 3 |
Li3AlFeO4 (mp-772439) | 0.5444 | 0.029 | 4 |
Li3MnAlO4 (mp-770591) | 0.6476 | 0.052 | 4 |
Li3AlNiO4 (mp-770491) | 0.4674 | 0.103 | 4 |
Li3MgNiO4 (mp-776903) | 0.6015 | 0.076 | 4 |
Li3AlCoO4 (mp-771900) | 0.5541 | 0.080 | 4 |
PbS (mp-1087486) | 0.7365 | 0.082 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv O |
Final Energy/Atom-5.0304 eV |
Corrected Energy-139.2191 eV
-139.2191 eV = -130.7916 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)