material

Ni2B

ID:

mp-2536

DOI:

10.17188/1200592


Tags: Nickel boride (2/1)

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.290 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.11 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 42532 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 0 0> <0 0 1> 0.000 24.6
C (mp-48) <1 1 1> <1 1 0> 0.006 269.3
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.008 196.8
Mg (mp-153) <1 1 0> <1 1 1> 0.010 116.2
Al (mp-134) <1 1 1> <1 0 0> 0.014 84.6
CsI (mp-614603) <1 0 0> <0 0 1> 0.017 123.0
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.018 84.6
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.020 275.1
C (mp-48) <0 0 1> <1 0 0> 0.022 21.2
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.024 97.3
ZnO (mp-2133) <0 0 1> <1 0 0> 0.025 84.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.026 221.4
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.030 123.0
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.035 275.1
BaF2 (mp-1029) <1 1 1> <1 0 0> 0.039 275.1
Te2W (mp-22693) <0 1 1> <1 1 1> 0.039 116.2
TePb (mp-19717) <1 0 0> <1 0 1> 0.040 129.8
CdWO4 (mp-19387) <1 1 1> <1 1 1> 0.044 154.9
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.045 275.1
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.050 196.8
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.057 123.0
Al (mp-134) <1 1 0> <1 1 0> 0.059 209.5
GaN (mp-804) <1 1 0> <1 1 1> 0.062 116.2
PbS (mp-21276) <1 1 0> <1 0 0> 0.067 253.9
PbS (mp-21276) <1 0 0> <1 1 0> 0.075 179.5
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.084 232.7
LiGaO2 (mp-5854) <1 0 1> <1 1 1> 0.084 271.1
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.088 196.8
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.090 123.0
SrTiO3 (mp-4651) <1 0 0> <1 1 1> 0.093 309.9
AlN (mp-661) <0 0 1> <1 0 1> 0.094 194.7
Ni (mp-23) <1 1 1> <0 0 1> 0.104 172.2
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.105 269.3
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.105 239.4
SiO2 (mp-6930) <1 1 0> <1 1 1> 0.108 193.7
TiO2 (mp-390) <1 1 0> <1 1 0> 0.110 209.5
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.110 221.4
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.112 221.4
Te2W (mp-22693) <0 0 1> <1 1 0> 0.118 89.8
Cu (mp-30) <1 1 1> <1 0 0> 0.121 275.1
GaN (mp-804) <1 1 1> <0 0 1> 0.122 123.0
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.122 84.6
YAlO3 (mp-3792) <1 0 0> <1 0 0> 0.123 317.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.124 209.5
LiGaO2 (mp-5854) <1 1 0> <1 0 1> 0.127 97.3
SiC (mp-7631) <1 0 0> <1 0 0> 0.129 232.7
GdScO3 (mp-5690) <0 0 1> <1 1 1> 0.129 193.7
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.130 119.7
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.136 123.0
MgO (mp-1265) <1 0 0> <1 1 0> 0.139 89.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
354 171 171 0 0 0
171 401 211 0 0 0
171 211 401 0 0 0
0 0 0 132 0 0
0 0 0 0 86 0
0 0 0 0 0 86
Compliance Tensor Sij (10-12Pa-1)
3.9 -1.1 -1.1 0 0 0
-1.1 3.7 -1.5 0 0 0
-1.1 -1.5 3.7 0 0 0
0 0 0 7.6 0 0
0 0 0 0 11.6 0
0 0 0 0 0 11.6
Shear Modulus GV
101 GPa
Bulk Modulus KV
251 GPa
Shear Modulus GR
98 GPa
Bulk Modulus KR
248 GPa
Shear Modulus GVRH
100 GPa
Bulk Modulus KVRH
250 GPa
Elastic Anisotropy
0.15
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.2238 0.053 3
Nb4SiNi (mp-22396) 0.3417 0.004 3
Ta4FeP (mp-22444) 0.2479 0.055 3
Nb4FeSi (mp-22312) 0.3502 0.048 3
Zr4CuP (mp-581733) 0.3562 0.063 3
Co2B (mp-1071320) 0.1036 0.024 2
BW2 (mp-1113) 0.0083 0.000 2
Co2B (mp-493) 0.0869 0.024 2
Ta2B (mp-1032) 0.0937 0.036 2
BMo2 (mp-2501) 0.0630 0.018 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv B
Final Energy/Atom
-6.3696 eV
Corrected Energy
-38.2176 eV
Uncorrected energy = -38.2176 eV Corrected energy = -38.2176 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 30448
  • 42532
  • 603804
  • 614977
  • 75792
  • 108072
  • 614984
Submitted by
User remarks:
  • Nickel boride (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)