Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.853 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.067 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(CO4)2 + LiPO3 + CO2 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 122.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 122.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 224.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 256.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 211.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 325.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 192.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 253.4 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 122.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 337.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 306.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 288.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 320.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 -1> | 223.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 223.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 206.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 256.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 160.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 256.6 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 122.6 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 306.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 256.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 211.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 306.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 295.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 224.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 32.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 224.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 160.4 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 223.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 323.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 320.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 -1> | 223.4 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 148.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 231.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 352.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 320.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 288.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 223.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 318.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 168.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 211.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 256.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 320.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 253.4 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 245.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 96.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 184.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9V19O48 (mp-777033) | 0.7253 | 0.102 | 3 |
Bi2B2O7 (mp-756526) | 0.6825 | 0.080 | 3 |
V2NiO6 (mp-32382) | 0.7398 | 0.019 | 3 |
CuSeO4 (mp-554040) | 0.7319 | 0.000 | 3 |
Li2Mg11(WO4)12 (mp-853222) | 0.6367 | 0.120 | 4 |
Li2Mo(PO4)2 (mp-540296) | 0.6385 | 0.063 | 4 |
Mg5V2(MoO8)2 (mp-646182) | 0.6475 | 0.023 | 4 |
LiBiB2O5 (mp-768665) | 0.6413 | 0.091 | 4 |
MnZnPO5 (mvc-3247) | 0.5887 | 0.029 | 4 |
NaSbAsCO7 (mp-768815) | 0.2171 | 0.098 | 5 |
NaSiSbCO7 (mp-772595) | 0.2750 | 0.059 | 5 |
NaMnPCO7 (mp-775526) | 0.2661 | 0.120 | 5 |
NaMnPCO7 (mp-769584) | 0.2404 | 0.123 | 5 |
NaSbPCO7 (mp-768121) | 0.2508 | 0.101 | 5 |
KLiMnPCO7 (mp-764256) | 0.7405 | 0.000 | 6 |
NaLiMnPCO7 (mp-763833) | 0.6660 | 0.062 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P C O |
Final Energy/Atom-6.4316 eV |
Corrected Energy-151.1139 eV
Uncorrected energy = -141.4959 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -151.1139 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)