Final Magnetic Moment2.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.807 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 |
Band Gap1.950 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 96.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 96.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 141.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 163.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 133.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 85.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 349.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 167.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 145.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 200.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 217.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 200.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 260.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 167.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 290.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 223.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 72.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 327.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 218.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 212.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 312.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 212.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 167.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 145.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 83.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 156.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 230.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 217.4 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 217.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 215.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 209.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 186.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 260.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 305.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 217.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr(CoO3)2 (mp-765852) | 0.2372 | 0.316 | 3 |
Co3NiO8 (mp-765936) | 0.2219 | 0.038 | 3 |
CrCo3O8 (mp-765865) | 0.2294 | 0.107 | 3 |
Mn(CoO3)2 (mp-763057) | 0.2365 | 0.065 | 3 |
FeCoO4 (mp-771871) | 0.2400 | 0.133 | 3 |
Ti2Mn3Cr3O16 (mp-771540) | 0.5586 | 0.084 | 4 |
Ti3Mn3Cr2O16 (mp-770915) | 0.5814 | 0.098 | 4 |
Mn3Cr3(WO8)2 (mp-778921) | 0.5438 | 0.103 | 4 |
LiV3(OF3)2 (mp-766156) | 0.5608 | 0.082 | 4 |
Mn3Cr3(TeO8)2 (mp-772458) | 0.5411 | 0.082 | 4 |
CoO2 (mp-554635) | 0.1549 | 0.007 | 2 |
CoO2 (mp-715472) | 0.1515 | 0.007 | 2 |
CeSe2 (mp-1080274) | 0.1758 | 0.063 | 2 |
CoO2 (mp-715478) | 0.1539 | 0.007 | 2 |
CeSe2 (mp-1098702) | 0.1600 | 0.063 | 2 |
Explore more synthesis descriptions for materials of composition MnO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv O |
Final Energy/Atom-7.1307 eV |
Corrected Energy-24.4776 eV
-24.4776 eV = -21.3922 eV (uncorrected energy) - 1.6809 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)