Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.403 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsMn2(PO3)6 + MnPO4 + MnP2O7 + CsP2H5O8 + CsPO3 |
Band Gap2.980 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <0 0 1> | <1 0 0> | 174.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 332.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 277.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 234.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 290.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 80.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 287.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 240.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 240.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 232.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 277.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 290.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 174.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 240.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 232.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 332.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 156.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 232.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 78.2 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 287.6 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 287.6 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 221.7 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 240.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 110.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 240.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 78.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 234.7 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 240.6 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 234.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 160.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 312.9 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 312.9 |
MgO (mp-1265) | <1 1 0> | <1 1 -1> | 287.6 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 78.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 160.4 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 332.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 174.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 290.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 58.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 58.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 290.0 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 257.3 |
C (mp-66) | <1 0 0> | <1 1 -1> | 191.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 160.4 |
C (mp-66) | <1 1 1> | <0 1 0> | 110.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 277.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 160.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 -1> | 312.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 174.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.13770 | 0.00000 | -0.08320 |
-0.07808 | -0.16741 | 0.07690 | 0.00000 | -0.04837 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.10863 | 0.00000 | -0.04323 |
Piezoelectric Modulus ‖eij‖max0.20586 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-2.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.02 | 0.00 | -0.26 |
0.00 | 3.07 | -0.00 |
-0.26 | -0.00 | 2.69 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.89 | 0.00 | 0.38 |
0.00 | 6.07 | -0.00 |
0.38 | -0.00 | 6.43 |
Polycrystalline dielectric constant
εpoly∞
2.93
|
Polycrystalline dielectric constant
εpoly
6.46
|
Refractive Index n1.71 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd2P6O17 (mp-29276) | 0.6743 | 0.000 | 3 |
VP2O7 (mp-565555) | 0.6551 | 0.151 | 3 |
RePO5 (mp-867296) | 0.6513 | 0.000 | 3 |
V3(P3O10)2 (mp-32524) | 0.6700 | 0.027 | 3 |
Fe3(P3O10)2 (mp-31877) | 0.6725 | 0.169 | 3 |
V2P4H3O16 (mp-771427) | 0.5594 | 0.077 | 4 |
Nb2P4H3O16 (mp-770824) | 0.5933 | 0.084 | 4 |
LiTi(PO3)4 (mp-758240) | 0.5979 | 0.067 | 4 |
Te2P4H3O16 (mp-755681) | 0.5989 | 0.075 | 4 |
RbAl3(P3O10)2 (mp-555621) | 0.5905 | 0.000 | 4 |
LiMnP3HO10 (mp-763744) | 0.1415 | 0.199 | 5 |
LiVP3HO10 (mp-763631) | 0.3708 | 0.080 | 5 |
LiMnP3HO10 (mp-851011) | 0.4258 | 0.176 | 5 |
CsGaP3HO10 (mp-703308) | 0.4647 | 0.000 | 5 |
KMnP3HO10 (mp-542842) | 0.3880 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Cs_sv Mn_pv P H O |
Final Energy/Atom-6.7976 eV |
Corrected Energy-117.2992 eV
Uncorrected energy = -108.7612 eV
Composition-based energy adjustment (-0.687 eV/atom x 10.0 atoms) = -6.8700 eV
Composition-based energy adjustment (-1.668 eV/atom x 1.0 atoms) = -1.6680 eV
Corrected energy = -117.2992 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)