Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.899 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.238 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoO2 |
Band Gap1.260 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 248.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 117.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 248.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.6 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 143.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 82.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 117.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 82.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 82.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 117.1 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 143.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 82.8 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 165.6 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 234.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 117.1 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 248.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 165.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 234.2 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 248.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 82.8 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 117.1 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 117.1 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 248.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 165.6 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 165.6 |
Fe2O3 (mp-24972) | <1 1 0> | <1 0 0> | 248.4 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 234.2 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 165.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiMn2O6 (mp-775831) | 0.2957 | 0.085 | 3 |
Mn3VO8 (mp-771844) | 0.2921 | 0.133 | 3 |
CrSbO4 (mp-771809) | 0.2241 | 0.120 | 3 |
TiMn3O8 (mp-771787) | 0.2930 | 0.075 | 3 |
Mn3SbO8 (mp-776354) | 0.2829 | 0.100 | 3 |
V3Cr3(WO8)2 (mp-775969) | 0.6053 | 0.098 | 4 |
Ti2Mn3Cr3O16 (mp-771540) | 0.6107 | 0.084 | 4 |
Mn3Cr3(WO8)2 (mp-778921) | 0.5857 | 0.103 | 4 |
LiV3(OF3)2 (mp-766156) | 0.6120 | 0.082 | 4 |
Mn3Cr3(TeO8)2 (mp-772458) | 0.5993 | 0.082 | 4 |
BiO2 (mvc-4274) | 0.1154 | 0.245 | 2 |
SbO2 (mvc-4245) | 0.0534 | 0.409 | 2 |
CrO2 (mp-25499) | 0.1289 | 0.208 | 2 |
PtO2 (mp-7868) | 0.1366 | 0.005 | 2 |
WO2 (mp-715467) | 0.1318 | 0.424 | 2 |
Explore more synthesis descriptions for materials of composition MoO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: O Mo_pv |
Final Energy/Atom-7.1680 eV |
Corrected Energy-105.7578 eV
-105.7578 eV = -86.0155 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)