Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.481 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiPO4 + LiF |
Band Gap4.229 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 216.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 225.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 108.3 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 189.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 197.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 230.3 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 190.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 172.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 153.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 253.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 223.8 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 151.7 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 204.4 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 151.7 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 149.2 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 0> | 238.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 270.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 111.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 261.1 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 255.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 151.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 172.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 261.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 299.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 262.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 338.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 366.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 270.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 140.9 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 190.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 253.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 225.4 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 270.7 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 216.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 186.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 299.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 112.7 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 255.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 253.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 225.4 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 287.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 324.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 197.2 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 0> | 333.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 281.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 84.5 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 270.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 253.6 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 140.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2FeS4 (mp-676013) | 0.5990 | 0.524 | 3 |
Fe4P2O9 (mp-637226) | 0.5788 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.6331 | 0.015 | 3 |
Na5AsO5 (mp-17816) | 0.6196 | 0.003 | 3 |
Ni4P2O9 (mp-771899) | 0.5678 | 0.037 | 3 |
Li3Fe2(PO5)2 (mp-767823) | 0.5862 | 0.338 | 4 |
Li5Ni2(PO4)3 (mp-764093) | 0.6240 | 0.045 | 4 |
Li3Mo(PO4)2 (mp-32048) | 0.5898 | 0.030 | 4 |
Li3Ni(PO4)2 (mp-32398) | 0.5586 | 0.079 | 4 |
Li3V2(SiO5)2 (mp-25644) | 0.5604 | 0.064 | 4 |
Li2MnPO4F (mp-776063) | 0.4908 | 0.024 | 5 |
Li2CoPO4F (mp-25488) | 0.2043 | 0.054 | 5 |
Li2MnPO4F (mp-25562) | 0.2233 | 0.045 | 5 |
Li2VPO4F (mp-25630) | 0.1670 | 0.036 | 5 |
Li2FePO4F (mp-25688) | 0.2237 | 0.040 | 5 |
Li2MnVP2(HO5)2 (mp-849445) | 0.7493 | 0.015 | 6 |
Li3MnVP2(O4F)2 (mp-763904) | 0.5493 | 0.034 | 6 |
Li3VCrP2(O4F)2 (mp-766992) | 0.5749 | 0.027 | 6 |
Li3VFeP2(HO5)2 (mp-765312) | 0.7485 | 0.139 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O F |
Final Energy/Atom-5.9533 eV |
Corrected Energy-234.2117 eV
-234.2117 eV = -214.3191 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)