Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.261 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.108 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + W |
Band Gap2.935 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 336.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 156.4 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 273.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 205.2 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 241.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 208.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 136.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 214.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 302.2 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 208.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 275.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 260.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 260.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 336.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 244.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 336.7 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 208.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 241.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 160.7 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 244.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 153.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.5 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 91.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 122.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 61.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 367.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 153.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 153.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 260.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 214.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 367.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 244.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 260.6 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 260.6 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 244.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 183.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 153.0 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 61.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 367.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 181.3 |
TiO2 (mp-2657) | <1 0 1> | <1 1 1> | 258.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 275.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 52.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 91.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 91.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 336.7 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 260.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 336.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FePO4 (mp-25001) | 0.3285 | 0.024 | 3 |
CrPO4 (mp-31750) | 0.2308 | 0.055 | 3 |
TiPO4 (mp-5839) | 0.3360 | 0.072 | 3 |
CoSO4 (mp-19198) | 0.3430 | 0.002 | 3 |
NiPO4 (mp-540008) | 0.2365 | 0.231 | 3 |
CrFe(PO4)2 (mp-861612) | 0.2353 | 2.251 | 4 |
FeNi3(PO4)4 (mp-775077) | 0.2842 | 0.089 | 4 |
VSn(PO4)2 (mp-766913) | 0.1871 | 0.081 | 4 |
CoSn(PO4)2 (mp-863848) | 0.2737 | 0.039 | 4 |
NiSn(PO4)2 (mp-763591) | 0.2464 | 0.030 | 4 |
CrO2 (mvc-11581) | 0.5940 | 0.351 | 2 |
VO2 (mp-777469) | 0.6106 | 0.038 | 2 |
Cr5O12 (mp-19575) | 0.6418 | 0.142 | 2 |
VO2 (mvc-6918) | 0.5335 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.5299 | 0.387 | 2 |
MnFeCo(PO4)3 (mp-763496) | 0.4237 | 0.026 | 5 |
Co2Ni3Sb(PO4)6 (mp-762172) | 0.3997 | 0.095 | 5 |
Fe2Ni3Sb(PO4)6 (mp-777420) | 0.4030 | 0.089 | 5 |
Mn3CrTe2(PO4)6 (mp-767922) | 0.4276 | 0.085 | 5 |
Mn3Cr2Sb(PO4)6 (mp-776056) | 0.4173 | 0.097 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6338 | 0.080 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5664 | 0.003 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6243 | 0.028 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6412 | 0.001 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5243 | 0.008 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: P W_pv O |
Final Energy/Atom-7.4280 eV |
Corrected Energy-206.9134 eV
-206.9134 eV = -178.2728 eV (uncorrected energy) - 17.4040 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)