Final Magnetic Moment0.157 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.228 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.878 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Fe2O5 + Fe2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 99.4 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 256.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 298.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 101.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 142.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 142.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 106.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 232.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 232.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 165.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 313.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 114.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 165.7 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 306.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 298.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 132.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 232.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 165.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 285.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 218.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 262.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 165.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 165.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 298.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 213.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 106.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 165.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 306.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 313.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 232.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 256.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 85.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 213.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 218.6 |
Te2W (mp-22693) | <1 1 0> | <0 1 1> | 218.6 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 306.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 306.0 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 213.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 85.5 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 298.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 199.5 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 285.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 285.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 370.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 285.1 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 349.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 298.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 165.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 85.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaSc2O4 (mp-4056) | 0.1093 | 0.000 | 3 |
SrIn2O4 (mp-540688) | 0.1095 | 0.000 | 3 |
CaV2O4 (mvc-12645) | 0.0957 | 0.000 | 3 |
Ca(GaO2)2 (mp-4959) | 0.0627 | 0.051 | 3 |
CaV2O4 (mp-540837) | 0.1019 | 0.000 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.7030 | 0.013 | 4 |
FeBiSbS4 (mp-601716) | 0.7206 | 0.170 | 4 |
Na3Mn4(TeO6)2 (mp-565229) | 0.5744 | 0.190 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ca_sv Fe_pv O |
Final Energy/Atom-5.8073 eV |
Corrected Energy-191.6434 eV
Uncorrected energy = -162.6034 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-2.256 eV/atom x 8.0 atoms) = -18.0480 eV
Corrected energy = -191.6434 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)