Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.128 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.094 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 55.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 196.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 267.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 229.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 209.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 279.2 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 285.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 55.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 167.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 32.8 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 285.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 327.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 167.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 55.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 279.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 89.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 163.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 229.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 32.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 77.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 278.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 229.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 279.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 229.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 163.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 229.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 209.1 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 323.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 279.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 229.3 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 267.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 65.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 98.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 267.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 327.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 231.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 139.4 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 231.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 285.4 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 194.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 267.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 262.0 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 258.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 229.3 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 98.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 258.9 |
YVO4 (mp-19133) | <1 0 1> | <1 1 1> | 285.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 65.5 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 258.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 258.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2SiO4 (mp-2895) | 0.1492 | 0.000 | 3 |
Be(FeO2)2 (mp-770566) | 0.1662 | 0.050 | 3 |
Co2SiO4 (mp-555558) | 0.1850 | 0.617 | 3 |
Si(NiO2)2 (mp-19072) | 0.1721 | 0.000 | 3 |
Mg2GeO4 (mp-3051) | 0.1819 | 0.000 | 3 |
LiCoAsO4 (mp-24861) | 0.1786 | 0.000 | 4 |
LiNiAsO4 (mp-25613) | 0.1469 | 0.000 | 4 |
LiInGeO4 (mp-17854) | 0.1318 | 0.000 | 4 |
CaLaGaO4 (mp-559969) | 0.1678 | 0.000 | 4 |
Mg7Fe(SiO4)4 (mp-1094131) | 0.1814 | 0.067 | 4 |
Si3N4 (mp-641539) | 0.4068 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4356 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.4253 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.2788 | 0.226 | 2 |
Fe3O4 (mp-650112) | 0.4541 | 0.060 | 2 |
Li4Co3Ni3(WO8)2 (mp-764321) | 0.3572 | 0.056 | 5 |
Li2CoNi(PO4)2 (mp-761996) | 0.3533 | 0.016 | 5 |
Li4V3Ni3(WO8)2 (mp-777059) | 0.3645 | 0.032 | 5 |
Li4V3Ni2Sn3O16 (mp-777392) | 0.3517 | 0.081 | 5 |
Li4V3Co3(WO8)2 (mp-763152) | 0.3600 | 0.263 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.4306 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.4291 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.4376 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.4341 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.4348 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Ge_d O |
Final Energy/Atom-7.3512 eV |
Corrected Energy-230.5160 eV
-230.5160 eV = -205.8326 eV (uncorrected energy) - 13.4468 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)