Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.512 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH2O + WSe2 + WO3 + N2 + Se |
Band Gap3.106 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 160.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 327.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 327.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 233.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 327.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 46.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 207.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 327.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 327.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 327.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 277.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 92.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 327.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 327.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 327.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 187.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 233.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 187.1 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 160.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 233.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 327.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 187.1 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 233.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 92.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 187.1 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 160.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 187.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 140.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 233.9 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 327.4 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 160.0 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 327.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 46.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 140.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 327.4 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 327.4 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 327.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 277.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 327.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 277.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 327.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 327.4 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 233.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 327.4 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 140.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 140.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 46.8 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 277.2 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 277.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.92305 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.92304 | 0.00000 | 0.00000 |
-0.04471 | -0.04471 | 0.59186 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.92305 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
-0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.37 | 0.00 | 0.00 |
0.00 | 4.37 | 0.00 |
0.00 | 0.00 | 3.25 |
Dielectric Tensor εij (total) |
||
---|---|---|
34.61 | 0.00 | -0.00 |
0.00 | 34.61 | -0.00 |
-0.00 | -0.00 | 6.71 |
Polycrystalline dielectric constant
εpoly∞
4.00
|
Polycrystalline dielectric constant
εpoly
25.31
|
Refractive Index n2.00 |
Potentially ferroelectric?Unknown |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: H N O Se W_pv |
Final Energy/Atom-6.2077 eV |
Corrected Energy-365.9179 eV
Uncorrected energy = -322.8019 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-4.438 eV/atom x 6.0 atoms) = -26.6280 eV
Corrected energy = -365.9179 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)