Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2SO4 + NiH2SO5 + H2O |
Band Gap4.871 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 236.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 281.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 305.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 325.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 150.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 111.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 216.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 76.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 216.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 216.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 305.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 76.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 270.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 150.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 305.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 325.1 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 259.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 152.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 229.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 152.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 222.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 325.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 270.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 305.7 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 236.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 162.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 -1> | 259.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 281.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 162.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 305.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 216.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 305.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 150.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 305.7 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 281.0 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 123.7 |
C (mp-66) | <1 0 0> | <0 1 1> | 281.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 325.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 281.0 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 270.9 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 325.1 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 216.7 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 281.0 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 270.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 325.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 325.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 305.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 305.7 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 216.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrPO4 (mp-850489) | 0.7213 | 0.067 | 3 |
Mg3(PO6)2 (mp-867981) | 0.7219 | 0.555 | 3 |
CrPO4 (mp-767021) | 0.7169 | 0.064 | 3 |
V4As2O13 (mp-32447) | 0.7335 | 0.000 | 3 |
V4P2O13 (mp-768034) | 0.7323 | 0.023 | 3 |
InP(H2O3)2 (mp-766835) | 0.4583 | 0.000 | 4 |
Mg3P2(HO)16 (mp-766572) | 0.4481 | 0.021 | 4 |
MnP2(H4O5)2 (mp-745106) | 0.4412 | 0.000 | 4 |
CoP2(H4O5)2 (mp-25477) | 0.4325 | 0.041 | 4 |
NiP2(H4O5)2 (mp-542954) | 0.4444 | 0.024 | 4 |
K2FeH12(SO7)2 (mp-543050) | 0.1335 | 0.048 | 5 |
K2MgH12(SO7)2 (mp-24438) | 0.1602 | 0.002 | 5 |
K2H12Ru(SO7)2 (mp-24538) | 0.1588 | 0.046 | 5 |
K2FeH12(SO7)2 (mp-565841) | 0.1610 | 0.048 | 5 |
K2NiH12(SO7)2 (mp-566571) | 0.1040 | 0.016 | 5 |
InBP2H5NO9 (mp-752709) | 0.6735 | 0.000 | 6 |
KNaZrSi3H4O11 (mp-773906) | 0.6023 | 0.000 | 6 |
CsKTeH6SO10 (mp-559375) | 0.6216 | 0.000 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6931 | 0.072 | 6 |
Be2CoH20N2(O3F4)2 (mp-25732) | 0.6248 | 0.000 | 6 |
Ca2AlH8S2Cl(O6F)2 (mp-643446) | 0.6192 | 0.001 | 7 |
K2NaCa2TiSi7HO20 (mp-720410) | 0.7255 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: K_sv Ni_pv H S O |
Final Energy/Atom-5.2639 eV |
Corrected Energy-353.0050 eV
-353.0050 eV = -326.3590 eV (uncorrected energy) - 22.3180 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)