Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.473 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.013 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 0 0> | <0 1 1> | 113.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 238.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 238.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 243.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 238.4 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 238.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 317.9 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 227.0 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 227.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 79.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 238.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 238.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 317.9 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 227.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 317.9 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 243.2 |
SiC (mp-11714) | <1 0 1> | <0 1 1> | 227.0 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 144.0 |
Au (mp-81) | <1 1 0> | <0 0 1> | 317.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 238.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 243.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 238.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 238.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 238.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 238.4 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 238.4 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 317.9 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 227.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 144.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 144.0 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 165.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 144.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 144.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 144.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 238.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 238.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 144.0 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 81.1 |
MgF2 (mp-1249) | <1 1 1> | <1 1 1> | 183.4 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 243.2 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 243.2 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 79.5 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 238.4 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 1> | 227.0 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 317.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnH10SeO9 (mp-542221) | 0.3099 | 0.016 | 4 |
MgH14SO11 (mp-24396) | 0.1133 | 0.009 | 4 |
MnH8SO8 (mp-25771) | 0.4235 | 0.018 | 4 |
MnH10SO9 (mp-541186) | 0.3014 | 0.017 | 4 |
AlH11SO10 (mp-722527) | 0.4558 | 0.000 | 4 |
Ge7H18O23 (mp-627442) | 0.6822 | 0.076 | 3 |
MgTlP(H6O5)2 (mp-554894) | 0.5101 | 0.000 | 5 |
LiMnP(H6O5)2 (mp-850407) | 0.5067 | 0.037 | 5 |
CoNiH24(SO10)2 (mp-542386) | 0.4156 | 0.006 | 5 |
Na2CoP4(H4O5)4 (mp-762847) | 0.5213 | 0.001 | 5 |
Li2CrP4(H4O5)4 (mp-763724) | 0.5309 | 0.015 | 5 |
AlCuH28S2ClO22 (mp-706670) | 0.4324 | 0.007 | 6 |
NiH24C2S2(N3O7)2 (mp-744811) | 0.6509 | 0.035 | 6 |
Be2CoH20N2(O3F4)2 (mp-25732) | 0.4460 | 0.000 | 6 |
AlZnH16N(OF)6 (mp-773079) | 0.6843 | 0.003 | 6 |
AlNiH16N(OF)6 (mp-773587) | 0.6728 | 0.001 | 6 |
K2NaCa2TiSi7HO20 (mp-720410) | 0.7333 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points2 |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: H O S Ni_pv |
Final Energy/Atom-5.1395 eV |
Corrected Energy-597.2795 eV
-597.2795 eV = -555.0689 eV (uncorrected energy) - 33.5546 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)