Final Magnetic Moment5.724 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.054 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 135.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 362.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 339.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 271.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 294.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 316.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 339.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 294.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 158.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 124.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 249.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 248.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 158.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 271.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 113.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 203.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 203.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 362.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 90.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 294.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 203.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 362.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 362.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 362.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 271.6 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 90.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 90.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 248.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 67.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 22.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 203.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 67.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 203.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 158.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 271.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 226.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 203.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 135.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 203.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbAl2Cu (mp-977428) | 0.1914 | 0.000 | 3 |
Gd3Al7Ag2 (mp-637182) | 0.2456 | 0.000 | 3 |
GdMg2Ni9 (mp-567249) | 0.2816 | 0.451 | 3 |
CaMg2Ni9 (mp-12695) | 0.2618 | 0.013 | 3 |
Ca3Al7Ag2 (mp-11430) | 0.1830 | 0.000 | 3 |
HoFe3 (mp-30634) | 0.0214 | 0.000 | 2 |
ErFe3 (mp-569783) | 0.0683 | 0.000 | 2 |
YbCo3 (mp-1095601) | 0.0940 | 0.000 | 2 |
ThFe3 (mp-30638) | 0.1329 | 0.205 | 2 |
ThFe3 (mp-1095695) | 0.1194 | 0.205 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Fe_pv |
Final Energy/Atom-7.5648 eV |
Corrected Energy-90.7775 eV
-90.7775 eV = -90.7775 eV (uncorrected energy)
|