Final Magnetic Moment0.993 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.191 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CuP2O7 + CuO |
Band Gap0.391 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 304.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 270.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 81.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 60.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 270.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 304.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 60.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 81.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 243.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 162.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 304.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 270.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 108.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 304.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 304.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 324.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 304.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 216.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 245.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 108.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 121.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 216.5 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 121.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 182.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 304.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 108.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 182.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 324.8 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 304.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 54.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 324.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 270.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 270.7 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 304.2 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 304.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 182.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 54.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 122.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 212.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 304.2 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 182.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 162.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 182.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 54.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 54.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 212.7 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 212.7 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 244.3 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 60.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca6Al7O16 (mp-721592) | 0.6153 | 0.000 | 3 |
Mn7SiO12 (mp-580307) | 0.6020 | 0.336 | 3 |
MnPO4 (mp-31942) | 0.5674 | 0.062 | 3 |
Na2MoO4 (mp-25068) | 0.6164 | 0.018 | 3 |
Cd2SiO4 (mp-4530) | 0.6486 | 0.000 | 3 |
LiNiPO4 (mp-765817) | 0.5326 | 0.072 | 4 |
LiCrPO4 (mp-540392) | 0.5555 | 0.731 | 4 |
LiCrPO4 (mp-31647) | 0.2544 | 0.042 | 4 |
LiCoPO4 (mp-761732) | 0.5107 | 0.070 | 4 |
LiCuPO4 (mp-584808) | 0.0944 | 0.037 | 4 |
Na2LiVPO6 (mp-763825) | 0.7470 | 0.094 | 5 |
Li2CrPO4F (mp-763748) | 0.7296 | 0.175 | 5 |
Li2MnPO4F (mp-762824) | 0.7281 | 0.039 | 5 |
Li4Nb2Fe3Te3O16 (mp-765556) | 0.7148 | 0.260 | 5 |
Na3Li2Al(SiO4)2 (mp-1020163) | 0.7210 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2485 eV |
Corrected Energy-92.9749 eV
Uncorrected energy = -87.4789 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -92.9749 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)