@article{Olson1966, author = "Olson, W.M. and Mulford, R.N.R.", title = "The melting point and decompostion pressure of neptunium mononitride", journal = "Journal of Physical Chemistry", year = "1966", volume = "70", pages = "2932-2934", ASTM_id = "JPCHAX" } @article{Lander1974, author = "Lander, G.H. and Mueller, M.H.", title = "Magnetically induced lattice distortions in actinide compounds", journal = "Physical Review, Serie 3. B - Solid State (1,1970-17,1977)", year = "1974", volume = "10", pages = "1994-2003", ASTM_id = "PLRBAQ" } @article{Shibata2010, author = "Shibata, H. and Tsuru, T. and Hirata, M. and Kaji, Y.", title = "First principles study on elastic properties and phase transition of Np N", journal = "Journal of Nuclear Materials", year = "2010", volume = "401", pages = "113-117", ASTM_id = "JNUMAM" } @article{Zachariasen1949, author = "Zachariasen, W.H.", title = "Crystal chemical studies of the 5f-series of elements XII.New compounds representing known structure types", journal = "Acta Crystallographica (1,1948-23,1967)", year = "1949", volume = "2", pages = "388-390", ASTM_id = "ACCRA9" } @article{Silva2012, author = "Silva, G.W.C. and Weck, P.F. and Eunja, Kim and Yeamans, C. B. and Cerefice, G. S. and Sattelberger, A.P. and Czerwinski, K.R.", title = "Crystal and electronic structures of neptunium nitrides synthesized using a fluoride route", journal = "Journal of the American Chemical Society", year = "2012", volume = "134", pages = "3111-3119", ASTM_id = "JACSAT" }