Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.327 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCu(PO3)3 + LiPO3 + Cu |
Band Gap2.229 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 279.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 143.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 279.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 326.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 106.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 114.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 279.6 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 143.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 186.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 279.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 114.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 247.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 247.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 326.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 260.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 106.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 208.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 312.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 208.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 326.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 229.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 312.4 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 212.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 208.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 312.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 312.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 326.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 186.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 279.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 326.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 326.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 229.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 106.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 208.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 208.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 312.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 208.3 |
Al (mp-134) | <1 1 1> | <0 1 0> | 326.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 326.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 143.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 326.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 312.4 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 312.4 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 326.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 260.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 326.4 |
SiC (mp-7631) | <1 0 0> | <1 1 -1> | 232.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 229.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 156.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 208.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-540419) | 0.5725 | 0.102 | 3 |
CuReO4 (mp-645206) | 0.5413 | 0.000 | 3 |
V2NiO6 (mp-1012103) | 0.4754 | 0.037 | 3 |
MnPO4 (mp-694547) | 0.6063 | 0.084 | 3 |
CuPO3 (mp-772255) | 0.3807 | 0.022 | 3 |
Li2FeP2O7 (mp-765934) | 0.5277 | 0.079 | 4 |
Li2CoP2O7 (mp-761663) | 0.5289 | 0.070 | 4 |
CsZnPO4 (mp-559752) | 0.5376 | 0.002 | 4 |
Rb2CdSi5O12 (mp-15125) | 0.5543 | 0.000 | 4 |
SiO2 (mp-556464) | 0.5296 | 0.241 | 2 |
SiO2 (mp-556553) | 0.6406 | 0.095 | 2 |
CeSe2 (mp-1080373) | 0.5443 | 0.531 | 2 |
CeSe2 (mp-1087553) | 0.6482 | 0.540 | 2 |
CrN2 (mp-1096894) | 0.5320 | 0.461 | 2 |
Cs2NaAl(PO4)2 (mp-581862) | 0.7479 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.5499 eV |
Corrected Energy-139.4252 eV
-139.4252 eV = -130.9977 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)