Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.151 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2P4O13 + BiPO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 1 -1> | 160.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 164.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 82.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 113.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 138.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 82.1 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 113.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 138.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 164.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 82.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 82.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 178.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 138.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 82.1 |
TeO2 (mp-2125) | <0 0 1> | <1 1 -1> | 160.1 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 246.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 164.3 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 226.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 82.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 138.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 164.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 164.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 -1> | 113.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 164.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 164.3 |
WS2 (mp-224) | <1 0 0> | <1 1 0> | 178.6 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 226.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 138.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 164.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 -1> | 113.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 1> | 197.2 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 164.3 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 164.3 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 246.4 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 164.3 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 138.3 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 246.4 |
GaTe (mp-542812) | <0 0 1> | <1 0 -1> | 226.9 |
GaTe (mp-542812) | <1 0 -1> | <1 0 -1> | 226.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
In2(SO4)3 (mp-9209) | 0.2681 | 0.003 | 3 |
Sn2(SO4)3 (mp-768943) | 0.2565 | 0.088 | 3 |
Ni2(SO4)3 (mp-779766) | 0.2563 | 0.021 | 3 |
Sb2(SO4)3 (mp-768457) | 0.2766 | 0.009 | 3 |
Bi2(PO4)3 (mp-26286) | 0.2386 | 0.081 | 3 |
MgCr3(SO4)6 (mp-772325) | 0.3820 | 0.219 | 4 |
MgCr7(SO4)12 (mp-777486) | 0.3590 | 0.111 | 4 |
Cr3Ni(SO4)6 (mp-776858) | 0.3533 | 0.004 | 4 |
ZnCr3(SO4)6 (mvc-16353) | 0.3532 | 0.006 | 4 |
MgCr3(SO4)6 (mvc-16581) | 0.3640 | 0.221 | 4 |
Cr5O12 (mp-773920) | 0.7273 | 0.000 | 2 |
Cr3O8 (mp-782705) | 0.6056 | 0.053 | 2 |
Cr3O8 (mp-641815) | 0.7436 | 0.140 | 2 |
Mo4O11 (mp-565865) | 0.7369 | 0.005 | 2 |
Cr3O8 (mp-557959) | 0.6837 | 0.048 | 2 |
MgCr3Se2(SO6)4 (mp-769544) | 0.3785 | 0.249 | 5 |
K2YbSn(PO4)3 (mp-677714) | 0.4712 | 0.017 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.3992 | 0.263 | 5 |
K2CoP2WO10 (mp-645301) | 0.5193 | 0.000 | 5 |
K2NiP2WO10 (mp-566161) | 0.5407 | 0.000 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.7286 | 0.009 | 6 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.7293 | 0.030 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6538 | 0.001 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi P O |
Final Energy/Atom-6.5607 eV |
Corrected Energy-479.8380 eV
-479.8380 eV = -446.1281 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)