Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.649 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.602 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Group2/m |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 105.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 293.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 293.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 330.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 63.9 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 176.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 140.2 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 58.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 210.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 175.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 160.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 280.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 35.0 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 255.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 140.2 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 58.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 94.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 213.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 140.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 235.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 47.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 160.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 175.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 94.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 175.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 280.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 188.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 293.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 160.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 280.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 285.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 283.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 175.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 320.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 140.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 235.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 267.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 255.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 213.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 320.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 175.2 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 191.7 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 319.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 140.2 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 63.9 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 267.2 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 117.5 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 235.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 283.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 175.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2SiO4 (mp-758006) | 0.4752 | 0.058 | 3 |
VSiO3 (mp-769952) | 0.4858 | 0.019 | 3 |
Li2SO4 (mp-558382) | 0.2561 | 0.055 | 3 |
Na2CrO4 (mp-18779) | 0.3551 | 0.000 | 3 |
Na2FeO4 (mp-19044) | 0.3703 | 0.062 | 3 |
LiMnPO4 (mp-31939) | 0.0609 | 0.021 | 4 |
LiNiPO4 (mp-32324) | 0.1240 | 0.009 | 4 |
NaCaVO4 (mp-566919) | 0.1493 | 0.075 | 4 |
LiCoPO4 (mp-585360) | 0.1514 | 0.037 | 4 |
LiVPO4 (mp-761338) | 0.0971 | 0.010 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.4414 | 0.029 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.4121 | 0.022 | 5 |
Li7Fe7P6(O8F)3 (mp-997551) | 0.4558 | 0.221 | 5 |
Li5CrP2(O4F)2 (mp-770679) | 0.5460 | 0.037 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.5351 | 0.080 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6766 | 0.008 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.1784 eV |
Corrected Energy-218.9599 eV