Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.480 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCu(PO3)3 + LiPO3 |
Band Gap0.825 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 248.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 207.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 103.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 206.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 181.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 252.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 274.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 274.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 252.1 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 274.9 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 126.1 |
Al (mp-134) | <1 0 0> | <0 1 0> | 274.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 248.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 274.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 -1> | 158.1 |
TeO2 (mp-2125) | <1 0 1> | <1 0 -1> | 158.1 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 274.9 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 126.1 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 274.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 207.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 206.1 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 206.1 |
Mg (mp-153) | <1 1 1> | <1 1 1> | 181.6 |
GaP (mp-2490) | <1 0 0> | <1 1 1> | 181.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 274.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 274.9 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 274.9 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 252.1 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 274.9 |
Si (mp-149) | <1 0 0> | <1 1 1> | 181.6 |
Si (mp-149) | <1 1 0> | <1 0 0> | 207.3 |
Si (mp-149) | <1 1 1> | <1 0 0> | 103.7 |
Au (mp-81) | <1 1 0> | <0 1 0> | 274.9 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 274.9 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 206.1 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 207.3 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 252.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 206.1 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 103.7 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 207.3 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 126.1 |
MgF2 (mp-1249) | <1 0 1> | <1 0 -1> | 158.1 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 124.4 |
SrTiO3 (mp-4651) | <1 0 1> | <0 1 0> | 274.9 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 206.1 |
CaF2 (mp-2741) | <1 0 0> | <1 1 1> | 181.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4(PO4)3 (mp-504357) | 0.6170 | 0.068 | 3 |
Cu4(PO4)3 (mp-26742) | 0.5559 | 0.029 | 3 |
Cr4(PO4)3 (mp-705240) | 0.6129 | 0.068 | 3 |
Mn2P3O10 (mp-31981) | 0.5483 | 0.029 | 3 |
Cr4(PO4)3 (mp-773959) | 0.6175 | 0.068 | 3 |
Li2Cr(PO3)4 (mp-697850) | 0.4641 | 0.025 | 4 |
Li2Ni(PO3)4 (mp-761497) | 0.4472 | 0.092 | 4 |
Li2Cr(PO3)4 (mp-540260) | 0.2326 | 0.028 | 4 |
Na2CuSi3O8 (mp-557123) | 0.4510 | 0.009 | 4 |
Na2Cu(PO3)4 (mp-557171) | 0.3553 | 0.000 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.5763 | 0.086 | 5 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.7142 | 0.010 | 5 |
NaCaGaSi2O7 (mp-698690) | 0.7138 | 0.668 | 5 |
Na6Al4Fe(Si4O13)2 (mp-42298) | 0.6944 | 0.001 | 5 |
Na6Al4Fe(Si4O13)2 (mp-705484) | 0.7069 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv O P Cu_pv |
Final Energy/Atom-6.7092 eV |
Corrected Energy-271.8050 eV
-271.8050 eV = -254.9500 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)