Final Magnetic Moment6.990 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.134 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + Li2CuP2O7 + CuO |
Band Gap0.275 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 -1> | 247.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 301.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 271.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 312.6 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 176.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 312.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 312.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 150.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 301.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 312.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 226.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 258.9 |
TePb (mp-19717) | <1 1 0> | <1 -1 0> | 176.9 |
BN (mp-984) | <0 0 1> | <1 1 0> | 125.5 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 247.6 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 271.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 234.4 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 258.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 271.6 |
Al (mp-134) | <1 0 0> | <0 1 0> | 312.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 165.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 301.5 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 165.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 271.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 226.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 312.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 226.1 |
TiO2 (mp-2657) | <1 1 0> | <1 -1 0> | 176.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 234.4 |
Mg (mp-153) | <1 0 0> | <1 -1 1> | 216.3 |
TiO2 (mp-2657) | <1 1 1> | <1 -1 0> | 88.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 301.5 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 312.6 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 312.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 301.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 301.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 150.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 -1> | 271.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 258.9 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 258.9 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 271.6 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 226.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 150.7 |
SiC (mp-11714) | <1 0 0> | <1 -1 1> | 216.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 -1> | 181.1 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 1> | 258.9 |
Au (mp-81) | <1 0 0> | <0 1 1> | 258.9 |
C (mp-48) | <0 0 1> | <0 1 1> | 258.9 |
C (mp-48) | <1 0 0> | <0 1 -1> | 247.6 |
C (mp-48) | <1 1 0> | <0 1 -1> | 165.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu3(PO4)2 (mp-4093) | 0.5430 | 0.000 | 3 |
Ni4P2O9 (mp-769618) | 0.6489 | 0.066 | 3 |
Na3Mo2N5 (mp-1029845) | 0.5875 | 0.000 | 3 |
Na3W2N5 (mp-1029565) | 0.5900 | 0.000 | 3 |
Cu4P2O9 (mp-5169) | 0.4756 | 0.034 | 3 |
Li2Cr5(Si2O7)2 (mp-868281) | 0.5302 | 0.000 | 4 |
LiCr4(PO4)3 (mp-504356) | 0.5243 | 0.925 | 4 |
Li6Cr9(PO4)8 (mp-31709) | 0.3589 | 0.019 | 4 |
Li6Ni9(PO4)8 (mp-766747) | 0.5701 | 0.064 | 4 |
Na6Cu9(PO4)8 (mp-560368) | 0.4131 | 0.001 | 4 |
Mn2Cu5P4(HO9)2 (mp-745163) | 0.7186 | 0.015 | 5 |
Li2PWO4F (mp-25728) | 0.7066 | 0.352 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2709 eV |
Corrected Energy-367.3735 eV
-367.3735 eV = -344.9002 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)