Final Magnetic Moment0.994 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.866 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2PO5 + Cu2P2O7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 230.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 306.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 264.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 306.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 306.9 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 252.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 306.9 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 230.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 264.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 88.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 230.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 230.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 146.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 306.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 306.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 264.5 |
MgO (mp-1265) | <1 1 1> | <1 0 -1> | 126.5 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 233.7 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 230.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 230.1 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 230.1 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 264.5 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 230.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 146.7 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 306.9 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 306.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 306.9 |
C (mp-48) | <1 0 0> | <1 0 0> | 176.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 306.9 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 264.5 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 306.9 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 88.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 306.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 306.9 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 230.1 |
MgF2 (mp-1249) | <1 0 1> | <1 1 0> | 233.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 264.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 306.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 146.7 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 233.7 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 264.5 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 230.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 264.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 230.1 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 230.1 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 0> | 306.9 |
CaF2 (mp-2741) | <1 1 0> | <0 1 0> | 306.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 -1> | 252.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4(PO4)3 (mp-504357) | 0.5193 | 0.784 | 3 |
Cr4(PO4)3 (mp-705240) | 0.5249 | 0.784 | 3 |
Cr3(PO4)2 (mp-579247) | 0.5291 | 0.089 | 3 |
V2Cu3O8 (mp-600273) | 0.6342 | 0.018 | 3 |
Cr4(PO4)3 (mp-773959) | 0.5065 | 0.784 | 3 |
Zn3Cu2(Si2O7)2 (mvc-4826) | 0.5028 | 0.092 | 4 |
LiMnP2O7 (mp-31916) | 0.5124 | 0.006 | 4 |
ZnCr2(PO4)2 (mvc-10010) | 0.4754 | 0.059 | 4 |
MgCr2(PO4)2 (mvc-10057) | 0.4930 | 0.048 | 4 |
ZnCu2(PO4)2 (mvc-9496) | 0.4240 | 0.053 | 4 |
Na3LiMg4(Si2O5)6 (mp-695366) | 0.7125 | 0.710 | 5 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.6718 | 0.043 | 5 |
Na6Al4Fe(Si4O13)2 (mp-42298) | 0.6572 | 0.000 | 5 |
Na6Al4Fe(Si4O13)2 (mp-705484) | 0.6108 | 0.033 | 5 |
Na6Al4Fe(Si4O13)2 (mp-698697) | 0.6965 | 0.043 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv P O |
Final Energy/Atom-6.2648 eV |
Corrected Energy-254.9183 eV
-254.9183 eV = -238.0633 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)