material

Sb2Rh

ID:

mp-2682

DOI:

10.17188/1201244


Tags: Rhodium antimony (1/2) Rhodium antimonide (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.590 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.004 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 43501 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <0 0 1> <1 0 1> 0.013 152.6
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.014 228.9
WS2 (mp-224) <0 0 1> <1 0 1> 0.015 228.9
Mg (mp-153) <0 0 1> <1 0 1> 0.016 228.9
BN (mp-984) <0 0 1> <1 0 1> 0.022 76.3
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.026 223.1
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.039 76.3
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.039 76.3
GaSe (mp-1943) <1 1 1> <1 0 -1> 0.046 236.7
GaSe (mp-1943) <0 0 1> <1 0 1> 0.055 76.3
GaSe (mp-1943) <1 1 0> <1 0 -1> 0.063 236.7
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.075 259.5
InP (mp-20351) <1 0 0> <0 0 1> 0.079 178.5
NaCl (mp-22862) <1 0 0> <1 1 1> 0.081 259.5
MgO (mp-1265) <1 1 0> <1 0 -1> 0.084 284.0
Al (mp-134) <1 0 0> <1 1 1> 0.092 259.5
LiF (mp-1138) <1 1 1> <1 0 1> 0.099 228.9
PbS (mp-21276) <1 0 0> <0 0 1> 0.106 178.5
MgAl2O4 (mp-3536) <1 1 1> <1 0 1> 0.116 228.9
C (mp-66) <1 0 0> <0 1 0> 0.126 204.0
BaTiO3 (mp-5986) <1 0 1> <1 1 -1> 0.130 187.5
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.134 152.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.135 223.1
Al (mp-134) <1 1 1> <1 0 1> 0.141 228.9
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.143 225.8
Mg (mp-153) <1 0 1> <0 1 0> 0.144 285.6
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.157 267.8
Te2Mo (mp-602) <1 0 0> <1 0 -1> 0.158 331.3
LiAlO2 (mp-3427) <1 0 1> <0 1 1> 0.161 302.3
Al (mp-134) <1 1 0> <1 0 1> 0.167 228.9
LiAlO2 (mp-3427) <1 0 0> <0 1 1> 0.184 302.3
AlN (mp-661) <1 1 1> <1 0 0> 0.188 225.8
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.196 225.8
ZnO (mp-2133) <1 1 0> <0 1 0> 0.196 122.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.197 44.6
AlN (mp-661) <1 0 0> <0 1 0> 0.202 326.4
CaCO3 (mp-3953) <0 0 1> <1 0 1> 0.202 152.6
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.202 243.4
TiO2 (mp-2657) <1 1 1> <1 0 -1> 0.204 236.7
InSb (mp-20012) <1 1 0> <1 0 -1> 0.210 189.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.220 89.3
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.223 312.4
TiO2 (mp-2657) <1 0 1> <0 1 0> 0.228 204.0
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.232 285.6
C (mp-66) <1 1 1> <1 0 1> 0.233 152.6
InSb (mp-20012) <1 0 0> <0 0 1> 0.235 44.6
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.238 259.5
KTaO3 (mp-3614) <1 1 1> <1 0 1> 0.241 228.9
CdTe (mp-406) <1 1 0> <1 0 -1> 0.242 189.3
ZnO (mp-2133) <1 0 0> <1 0 -1> 0.252 142.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
180 54 64 0 25 0
54 229 59 0 13 0
64 59 184 0 -10 0
0 0 0 73 0 22
25 13 -10 0 49 0
0 0 0 22 0 52
Compliance Tensor Sij (10-12Pa-1)
7.2 -0.8 -2.5 0 -4 0
-0.8 5 -1.4 0 -1.2 0
-2.5 -1.4 6.9 0 3.1 0
0 0 0 15.5 0 -6.4
-4 -1.2 3.1 0 23.6 0
0 0 0 -6.4 0 21.7
Shear Modulus GV
63 GPa
Bulk Modulus KV
105 GPa
Shear Modulus GR
54 GPa
Bulk Modulus KR
102 GPa
Shear Modulus GVRH
58 GPa
Bulk Modulus KVRH
104 GPa
Elastic Anisotropy
0.82
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CoGeTe (mp-3715) 0.3817 0.000 3
GeTeRh (mp-607818) 0.3926 0.048 3
FeAsS (mp-561511) 0.3792 0.000 3
PRuS (mp-1095584) 0.4082 0.005 3
TeAsRu (mp-1095634) 0.3295 0.000 3
Li8Mn(O2F)2 (mp-780086) 0.6411 0.071 4
Sr2Li2NiO4 (mp-769674) 0.5760 0.091 4
Na2Li3CoO4 (mp-540990) 0.6815 0.000 4
Li3CaMnN3 (mp-569112) 0.7180 0.000 4
LiCaGaN2 (mp-570948) 0.6576 0.000 4
CoSb2 (mp-755) 0.2060 0.002 2
Bi2Rh (mp-23217) 0.1702 0.000 2
CoAs2 (mp-2715) 0.1310 0.000 2
CoP2 (mp-14285) 0.2125 0.000 2
Sb2Ir (mp-1247) 0.1732 0.000 2
NaZr2SN2Cl (mp-679669) 0.6549 0.077 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sb Rh_pv
Final Energy/Atom
-5.6693 eV
Corrected Energy
-69.5681 eV
Uncorrected energy = -68.0321 eV Composition-based energy adjustment (-0.192 eV/atom x 8.0 atoms) = -1.5360 eV Corrected energy = -69.5681 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43501
  • 650241
  • 659978
  • 650245
  • 650249
Submitted by
User remarks:
  • Rhodium antimonide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)