Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.251 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58322 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.000 94.4
LiF (mp-1138) <1 1 0> <1 1 0> 0.000 47.2
KCl (mp-23193) <1 1 0> <1 1 0> 0.003 173.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.004 144.6
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.004 278.1
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.005 100.1
PbS (mp-21276) <1 1 1> <1 1 1> 0.005 250.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.007 77.1
SiC (mp-11714) <0 0 1> <1 1 1> 0.007 57.8
SiC (mp-7631) <0 0 1> <1 1 1> 0.010 57.8
Ge (mp-32) <1 1 0> <1 1 0> 0.011 47.2
Ge (mp-32) <1 1 1> <1 1 1> 0.011 57.8
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.014 251.7
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.018 141.6
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.020 144.6
InP (mp-20351) <1 1 0> <1 1 0> 0.024 298.9
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.024 55.6
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.027 125.9
LiAlO2 (mp-3427) <1 1 1> <1 1 1> 0.027 269.7
Mg (mp-153) <1 1 0> <1 1 0> 0.029 173.1
Si (mp-149) <1 1 0> <1 1 0> 0.030 125.9
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.032 141.6
LaAlO3 (mp-2920) <1 1 1> <1 1 0> 0.032 125.9
Te2W (mp-22693) <0 1 0> <1 0 0> 0.035 322.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.036 55.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.038 22.2
GaAs (mp-2534) <1 1 0> <1 1 0> 0.038 47.2
GaAs (mp-2534) <1 1 1> <1 1 1> 0.040 57.8
CsI (mp-614603) <1 1 0> <1 1 0> 0.041 173.1
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.045 78.7
InSb (mp-20012) <1 0 0> <1 0 0> 0.051 44.5
InSb (mp-20012) <1 1 0> <1 1 0> 0.056 62.9
LiF (mp-1138) <1 1 1> <1 0 0> 0.057 233.6
InSb (mp-20012) <1 1 1> <1 1 1> 0.058 77.1
LaF3 (mp-905) <0 0 1> <1 1 1> 0.062 134.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.063 44.5
BN (mp-984) <0 0 1> <1 1 0> 0.063 110.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.064 47.2
GaSe (mp-1943) <0 0 1> <1 1 0> 0.066 62.9
GaN (mp-804) <1 1 0> <1 1 0> 0.066 173.1
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.066 110.1
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.066 57.8
CdTe (mp-406) <1 1 0> <1 1 0> 0.070 62.9
CdTe (mp-406) <1 1 1> <1 1 1> 0.072 77.1
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.077 77.1
LiF (mp-1138) <1 0 0> <1 1 1> 0.078 134.9
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.078 178.0
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.080 289.2
TiO2 (mp-390) <1 0 1> <1 1 0> 0.088 361.8
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.088 125.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
85 55 55 0 0 0
55 85 55 0 0 0
55 55 85 0 0 0
0 0 0 48 0 0
0 0 0 0 48 0
0 0 0 0 0 48
Compliance Tensor Sij (10-12Pa-1)
24.1 -9.5 -9.5 0 0 0
-9.5 24.1 -9.5 0 0 0
-9.5 -9.5 24.1 0 0 0
0 0 0 20.9 0 0
0 0 0 0 20.9 0
0 0 0 0 0 20.9
Shear Modulus GV
35 GPa
Bulk Modulus KV
65 GPa
Shear Modulus GR
25 GPa
Bulk Modulus KR
65 GPa
Shear Modulus GVRH
30 GPa
Bulk Modulus KVRH
65 GPa
Elastic Anisotropy
1.83
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HoTmZn2 (mp-983126) 0.0000 0.000 3
Pm2PtAu (mp-982772) 0.0000 0.000 3
Nd2IrAu (mp-973606) 0.0000 0.057 3
YbPrPd2 (mp-981530) 0.0000 0.011 3
YTmAl2 (mp-980662) 0.0000 0.016 3
TiFeCoSb (mp-998973) 0.0000 0.186 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
VFeCoSi (mp-1066609) 0.0000 0.002 4
VFeCoSb (mp-1066862) 0.0000 0.163 4
ErPd (mp-851) 0.0000 0.000 2
YbRu (mp-567116) 0.0000 0.294 2
PrIn (mp-20023) 0.0000 0.000 2
ReC (mp-1009731) 0.0000 1.115 2
ScCu (mp-1169) 0.0000 0.000 2
Cu (mp-998890) 0.0000 0.037 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 2.271 1
Ge (mp-998883) 0.0000 0.339 1
U (mp-108) 0.0000 0.269 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Ag
Final Energy/Atom
-2.4671 eV
Corrected Energy
-4.9342 eV
Uncorrected energy = -4.9342 eV Corrected energy = -4.9342 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 605551
  • 184205
  • 605549
  • 150831
  • 605541
  • 151379
  • 605539
  • 605538
  • 605540
  • 58322
Submitted by
User remarks:
  • Silver magnesium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)