material

YCu2

ID:

mp-2698

DOI:

10.17188/1201271


Tags: Yttrium copper (1/2) Copper yttrium (2/1) Yttrium cupride (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.261 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Imma [74]
Hall
-I 2b 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 604016 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.004 290.5
TeO2 (mp-2125) <1 1 0> <1 1 0> 0.006 296.5
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.008 177.9
C (mp-48) <0 0 1> <0 1 0> 0.013 31.5
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.014 177.9
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.015 321.5
GaN (mp-804) <0 0 1> <0 1 0> 0.025 63.0
ZnO (mp-2133) <1 0 0> <0 1 0> 0.026 157.6
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.028 200.9
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.028 200.9
ZnO (mp-2133) <1 1 0> <1 1 1> 0.030 330.5
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.032 232.4
Mg (mp-153) <1 1 0> <0 1 0> 0.034 346.8
PbS (mp-21276) <1 0 0> <0 1 0> 0.037 252.2
C (mp-66) <1 1 0> <0 1 1> 0.040 214.9
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.044 220.7
Mg (mp-153) <1 0 0> <1 0 1> 0.047 116.2
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.053 251.1
SiC (mp-11714) <1 1 0> <0 1 1> 0.053 214.9
MgO (mp-1265) <1 0 0> <0 1 0> 0.056 126.1
CdS (mp-672) <1 1 0> <1 0 0> 0.056 50.2
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.060 174.3
InP (mp-20351) <1 1 0> <0 1 0> 0.064 252.2
AlN (mp-661) <1 1 0> <0 1 0> 0.066 189.1
PbS (mp-21276) <1 1 1> <0 1 0> 0.066 63.0
BN (mp-984) <1 0 0> <0 1 1> 0.071 214.9
TiO2 (mp-390) <1 0 0> <0 1 0> 0.072 220.7
LiAlO2 (mp-3427) <0 0 1> <0 1 0> 0.078 220.7
Al (mp-134) <1 0 0> <0 0 1> 0.081 263.1
WS2 (mp-224) <1 0 0> <0 0 1> 0.085 321.5
CdWO4 (mp-19387) <0 1 0> <0 1 0> 0.089 157.6
LiF (mp-1138) <1 1 0> <0 1 1> 0.092 214.9
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.096 157.6
LaF3 (mp-905) <1 0 1> <0 1 0> 0.096 283.7
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.099 204.6
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.103 204.6
Ga2O3 (mp-886) <1 0 -1> <0 1 0> 0.103 346.8
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.104 232.4
LiAlO2 (mp-3427) <1 1 0> <0 1 0> 0.110 94.6
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.113 132.2
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.114 157.6
ZnO (mp-2133) <1 0 1> <1 1 1> 0.115 198.3
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.116 177.9
CdS (mp-672) <1 0 1> <1 1 1> 0.117 66.1
PbS (mp-21276) <1 1 0> <0 1 0> 0.118 252.2
YVO4 (mp-19133) <1 1 0> <0 1 1> 0.118 129.0
BN (mp-984) <1 0 1> <0 1 1> 0.119 257.9
TbScO3 (mp-31119) <1 1 1> <0 1 1> 0.120 214.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.121 263.1
GdScO3 (mp-5690) <1 1 1> <0 1 1> 0.122 214.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
106 50 54 0 0 0
50 121 85 0 0 0
54 85 128 0 0 0
0 0 0 28 0 0
0 0 0 0 15 0
0 0 0 0 0 16
Compliance Tensor Sij (10-12Pa-1)
12.5 -2.9 -3.4 0 0 0
-2.9 16.1 -9.5 0 0 0
-3.4 -9.5 15.5 0 0 0
0 0 0 35.1 0 0
0 0 0 0 66.2 0
0 0 0 0 0 61.8
Shear Modulus GV
23 GPa
Bulk Modulus KV
81 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
79 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
0.62
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TbNiGe (mp-21424) 0.2721 0.000 3
SmGePt (mp-20293) 0.2553 0.013 3
ErNiGe (mp-20676) 0.3033 0.000 3
TmNiGe (mp-21157) 0.2775 0.000 3
HoNiGe (mp-542171) 0.1804 0.000 3
GdCu2 (mp-1077933) 0.0803 0.000 2
EuCu2 (mp-1071732) 0.1094 0.000 2
TbCu2 (mp-1527) 0.0681 0.000 2
NdCu2 (mp-11852) 0.1149 0.000 2
SmCu2 (mp-1077154) 0.0720 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cu_pv
Final Energy/Atom
-5.1494 eV
Corrected Energy
-30.8961 eV
-30.8961 eV = -30.8961 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 629429
  • 604016
  • 240071
  • 103143
Submitted by
User remarks:
  • Yttrium cupride (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)