Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.572 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4P2O7 + LiPO3 + Sn3(PO4)2 |
Band Gap3.936 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 289.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 289.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 167.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 93.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 167.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 289.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 167.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 93.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 279.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 192.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 167.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 289.5 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 192.4 |
BN (mp-984) | <1 0 0> | <1 0 1> | 192.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 93.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 186.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 279.1 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 289.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 186.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 289.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 193.0 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 289.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 93.0 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 279.1 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 93.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 279.1 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 279.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 186.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 186.1 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 289.5 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 289.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 1> | 192.4 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 186.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 289.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 279.1 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 289.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 186.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 193.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 279.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 279.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 1> | 134.0 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 289.5 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 0> | 289.5 |
MgF2 (mp-1249) | <1 0 1> | <0 1 1> | 134.0 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 279.1 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 167.3 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 93.0 |
Al2O3 (mp-1143) | <1 0 0> | <0 1 0> | 193.0 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 289.5 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 279.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4(PO4)3 (mp-704185) | 0.6143 | 0.097 | 3 |
Na2V2O5 (mp-780306) | 0.5794 | 0.141 | 3 |
CuPO3 (mp-766856) | 0.5568 | 0.090 | 3 |
Ag7P3S11 (mp-683910) | 0.5797 | 0.019 | 3 |
LiBeH3 (mp-24818) | 0.5559 | 0.006 | 3 |
Li2SnP2O7 (mp-758299) | 0.4277 | 0.066 | 4 |
LiBiB2O5 (mp-768776) | 0.4442 | 0.068 | 4 |
Li2SnP2O7 (mp-26407) | 0.4578 | 0.022 | 4 |
Li2CoP2O7 (mp-761664) | 0.4926 | 0.043 | 4 |
Li2FeP2O7 (mp-761456) | 0.4544 | 0.177 | 4 |
KNa3Al4(GeO4)4 (mp-573281) | 0.7451 | 0.336 | 5 |
NaCaGaSi2O7 (mp-698690) | 0.7227 | 0.666 | 5 |
AlSn3Se2ClO8 (mvc-1297) | 0.7210 | 0.258 | 5 |
NaLi2B(PO4)2 (mp-1020646) | 0.7316 | 0.000 | 5 |
RbZn2P2HO8 (mp-24683) | 0.7340 | 0.000 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.6988 | 0.223 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.6016 eV |
Corrected Energy-336.1107 eV
Uncorrected energy = -316.8747 eV
Composition-based energy adjustment (-0.687 eV/atom x 28.0 atoms) = -19.2360 eV
Corrected energy = -336.1107 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)