Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.426 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 221.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 77.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 77.2 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 110.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 311.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 141.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 310.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 340.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 270.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 145.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 115.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 217.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 155.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 141.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 85.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 255.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 155.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 217.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 311.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 145.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 217.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 207.1 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 290.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 283.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 145.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 193.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 155.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 217.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 193.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 115.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 217.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 270.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 166.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 145.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 193.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 270.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 231.7 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 166.1 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 55.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 270.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 193.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 290.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 113.4 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 283.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 77.2 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 283.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 311.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 177.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 191.6 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 221.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2Ag7 (mp-569486) | 0.2500 | 0.000 | 2 |
Ca2Ag7 (mp-16770) | 0.2299 | 0.000 | 2 |
Hf2Co7 (mp-1079776) | 0.1153 | 0.008 | 2 |
URe2 (mp-569480) | 0.7260 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Ni_pv |
Final Energy/Atom-6.8211 eV |
Corrected Energy-61.3903 eV
-61.3903 eV = -61.3903 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)