Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.523 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.782 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 309.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 306.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 230.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 142.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 309.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 197.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 309.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 185.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 230.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 230.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 185.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 230.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 185.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 230.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 230.1 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 185.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 230.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 230.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 295.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 309.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 142.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 309.3 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 295.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 309.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 185.6 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 295.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 306.8 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 230.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 247.4 |
Al (mp-134) | <1 1 1> | <1 0 0> | 230.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 295.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 142.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 185.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 230.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 185.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 230.1 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 148.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 76.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 76.7 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 230.1 |
C (mp-66) | <1 0 0> | <1 1 0> | 295.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 230.1 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 185.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 185.6 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 309.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 230.1 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 -1> | 142.8 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 142.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 185.6 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 230.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3SbO4 (mp-7404) | 0.4905 | 0.000 | 3 |
Na4WO5 (mp-19334) | 0.3511 | 0.000 | 3 |
Na4TeO5 (mp-15391) | 0.3497 | 0.000 | 3 |
Na3FeO4 (mp-778416) | 0.4337 | 0.009 | 3 |
Na3FeO4 (mp-764457) | 0.3988 | 0.143 | 3 |
Li3CrSiO5 (mp-762413) | 0.5009 | 0.197 | 4 |
Li3VSiO5 (mp-861563) | 0.4885 | 0.147 | 4 |
Li5V3(NiO5)2 (mp-851083) | 0.5414 | 0.139 | 4 |
Li2VO2F (mp-763225) | 0.5377 | 0.103 | 4 |
Na3LiMn5O9 (mp-762649) | 0.5330 | 0.338 | 4 |
Te2Au (mp-20123) | 0.5849 | 0.000 | 2 |
Te2Au (mp-571547) | 0.5621 | 0.010 | 2 |
Bi4I (mp-583234) | 0.6721 | 0.040 | 2 |
Bi9I2 (mp-28149) | 0.6735 | 0.027 | 2 |
FeS (mp-849091) | 0.7144 | 0.389 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Nb_pv O |
Final Energy/Atom-6.4009 eV |
Corrected Energy-216.0667 eV
-216.0667 eV = -204.8300 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)