Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.612 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTl3Cd2I7 + CdI2 |
Band Gap2.425 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 280.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 187.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 173.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 280.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 188.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 280.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 280.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 188.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 224.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 299.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 327.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 188.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 224.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 327.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 173.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 327.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 327.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 173.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 327.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 327.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 327.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 327.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 264.7 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 179.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 140.3 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 140.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 327.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 173.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 173.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 188.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 280.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 233.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 299.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 233.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 280.5 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 176.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 187.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 280.5 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 188.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 327.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 149.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 327.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 140.3 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 173.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 187.0 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 188.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 280.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 173.0 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 327.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 327.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnInBr3 (mp-28912) | 0.2871 | 0.004 | 3 |
CdInBr3 (mp-505222) | 0.2173 | 0.008 | 3 |
TlGeI3 (mp-29288) | 0.2581 | 0.016 | 3 |
SrZrSe3 (mp-541570) | 0.2503 | 0.027 | 3 |
TlCdBr3 (mp-28219) | 0.2640 | 0.001 | 3 |
Ca2CoRhO6 (mvc-13129) | 0.6633 | 0.209 | 4 |
Ca5Mn2(NiO6)2 (mvc-13112) | 0.6178 | 0.106 | 4 |
Ca2MnNiO6 (mvc-10906) | 0.6635 | 0.317 | 4 |
Ca2FeRhO6 (mvc-14247) | 0.6748 | 0.298 | 4 |
Ca3Co2(RhO6)2 (mvc-14984) | 0.6753 | 0.261 | 4 |
Ca5Gd3Ti5Mn3O24 (mp-744410) | 0.7265 | 0.013 | 5 |
Na3HoTi2Nb2O12 (mp-676988) | 0.7211 | 0.009 | 5 |
LiCaPrTeO6 (mp-40186) | 0.6866 | 0.024 | 5 |
CaPr2Ti2ZnO9 (mp-686602) | 0.6927 | 0.026 | 5 |
CaNd2Ti2ZnO9 (mp-677231) | 0.6965 | 0.034 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Cd I |
Final Energy/Atom-2.1798 eV |
Corrected Energy-43.5969 eV
-43.5969 eV = -43.5969 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)