Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.865 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.774 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 194.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 263.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 318.0 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 263.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 194.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 190.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 318.0 |
AlN (mp-661) | <0 0 1> | <1 1 -1> | 262.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 190.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 318.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 263.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 318.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 194.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 190.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 318.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 318.0 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 263.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 318.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 263.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 318.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 254.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 254.4 |
GaSe (mp-1943) | <1 0 1> | <1 0 -1> | 263.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 292.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 318.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 263.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 318.0 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 175.6 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 263.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 318.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 127.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 263.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 194.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 291.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 97.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 254.4 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 318.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 318.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 318.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 194.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 -1> | 263.4 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 263.4 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 263.4 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 190.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 194.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 254.4 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 254.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 194.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.37 | 0.00 | -0.21 |
0.00 | 7.13 | 0.00 |
-0.21 | 0.00 | 8.93 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.32 | 0.00 | -0.44 |
0.00 | 18.26 | 0.00 |
-0.44 | 0.00 | 14.86 |
Polycrystalline dielectric constant
εpoly∞
6.48
|
Polycrystalline dielectric constant
εpoly
13.48
|
Refractive Index n2.55 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KAuI3 (mp-31045) | 0.3720 | 0.000 | 3 |
La2CuO4 (mp-673846) | 0.6792 | 0.078 | 3 |
La2CuO4 (mp-19735) | 0.6667 | 0.071 | 3 |
RbAuI3 (mp-568666) | 0.2114 | 0.000 | 3 |
Rb2CuCl4 (mp-23508) | 0.6564 | 0.007 | 3 |
LiLa7(CuO7)2 (mp-775959) | 0.6737 | 0.033 | 4 |
LiLa8Cu3O16 (mp-774793) | 0.6608 | 0.052 | 4 |
Ba2Tl2CuO6 (mp-6027) | 0.6168 | 0.006 | 4 |
Sr2Cu(BiO3)2 (mp-555827) | 0.5932 | 0.059 | 4 |
Ba2Tl2CuO6 (mp-550722) | 0.6120 | 0.010 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Au Br |
Final Energy/Atom-2.6978 eV |
Corrected Energy-30.1825 eV
Uncorrected energy = -26.9785 eV
Composition-based energy adjustment (-0.534 eV/atom x 6.0 atoms) = -3.2040 eV
Corrected energy = -30.1825 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)