material

BaBr2

ID:

mp-27456

DOI:

10.17188/1201680


Tags: Barium dibromide Barium bromide

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.225 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.373 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 15706 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <0 1 0> 0.002 204.7
C (mp-66) <1 0 0> <0 1 0> 0.002 51.2
InP (mp-20351) <1 0 0> <0 0 1> 0.003 213.2
GdScO3 (mp-5690) <1 1 0> <0 1 0> 0.003 255.9
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.006 95.0
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.007 266.4
TbScO3 (mp-31119) <1 1 0> <0 1 0> 0.010 255.9
CdWO4 (mp-19387) <0 0 1> <0 1 0> 0.019 153.5
C (mp-48) <1 0 1> <0 0 1> 0.022 341.1
BN (mp-984) <0 0 1> <0 1 0> 0.024 153.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.027 255.8
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.027 213.2
GaSe (mp-1943) <0 0 1> <0 1 1> 0.029 199.8
DyScO3 (mp-31120) <1 1 0> <0 1 0> 0.031 255.9
AlN (mp-661) <1 0 1> <1 0 1> 0.031 285.0
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.031 42.6
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.032 215.8
MgF2 (mp-1249) <1 0 0> <0 1 1> 0.034 333.1
ZnO (mp-2133) <1 0 1> <0 0 1> 0.034 298.5
Au (mp-81) <1 1 0> <0 0 1> 0.034 298.5
CdS (mp-672) <1 0 0> <1 0 1> 0.035 285.0
C (mp-66) <1 1 0> <0 0 1> 0.037 127.9
WSe2 (mp-1821) <1 0 1> <0 0 1> 0.039 255.8
Cu (mp-30) <1 1 0> <0 0 1> 0.039 127.9
PbS (mp-21276) <1 1 0> <1 0 0> 0.040 254.6
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.040 215.8
TeO2 (mp-2125) <0 0 1> <0 1 0> 0.040 255.9
BaTiO3 (mp-5986) <1 1 1> <0 0 1> 0.042 85.3
LiGaO2 (mp-5854) <1 1 1> <0 1 1> 0.046 333.1
NaCl (mp-22862) <1 0 0> <0 1 0> 0.047 255.9
YAlO3 (mp-3792) <1 1 1> <1 0 1> 0.051 190.0
WSe2 (mp-1821) <1 0 0> <0 1 1> 0.051 199.8
MgO (mp-1265) <1 1 0> <1 0 0> 0.051 254.6
LiF (mp-1138) <1 1 1> <0 1 0> 0.054 204.7
AlN (mp-661) <1 1 0> <0 0 1> 0.055 298.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.058 341.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.059 213.2
ZnO (mp-2133) <1 1 1> <0 1 0> 0.060 255.9
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.070 254.6
Ag (mp-124) <1 1 0> <0 0 1> 0.070 298.5
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.070 255.9
Ge (mp-32) <1 1 0> <0 1 1> 0.074 333.1
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.080 204.7
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.082 204.7
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.083 204.7
LiGaO2 (mp-5854) <0 1 0> <0 1 1> 0.085 66.6
Al2O3 (mp-1143) <0 0 1> <1 0 1> 0.086 285.0
AlN (mp-661) <1 0 0> <0 0 1> 0.086 127.9
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.086 298.5
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.091 341.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
35 15 15 0 0 0
15 36 14 0 0 0
15 14 28 0 0 0
0 0 0 4 0 0
0 0 0 0 12 0
0 0 0 0 0 7
Compliance Tensor Sij (10-12Pa-1)
39.2 -10.2 -15.7 0 0 0
-10.2 36.4 -12 0 0 0
-15.7 -12 49.3 0 0 0
0 0 0 248.7 0 0
0 0 0 0 81.7 0
0 0 0 0 0 147.5
Shear Modulus GV
8 GPa
Bulk Modulus KV
21 GPa
Shear Modulus GR
7 GPa
Bulk Modulus KR
20 GPa
Shear Modulus GVRH
8 GPa
Bulk Modulus KVRH
21 GPa
Elastic Anisotropy
0.84
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KRbS (mp-28760) 0.4121 0.008 3
MoPRu (mp-22451) 0.4760 0.000 3
PbBrCl (mp-22997) 0.3768 0.010 3
VAsRh (mp-934092) 0.3489 0.002 3
VAsRh (mp-20395) 0.3247 0.002 3
Yb3In3Ge2Au (mp-981207) 0.7065 0.000 4
Na2LiGaAs2 (mp-9722) 0.6518 0.000 4
KNa4SnSb3 (mp-6758) 0.6919 0.005 4
K3Na2SnBi3 (mp-568329) 0.6906 0.000 4
LiCa2InGe2 (mp-570850) 0.7207 0.000 4
BaI2 (mp-23260) 0.0810 0.000 2
Cs2Te (mp-573763) 0.1718 0.000 2
BaF2 (mp-555585) 0.1648 0.040 2
Cs2Se (mp-1011696) 0.1702 0.020 2
BaCl2 (mp-23199) 0.0404 0.024 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Br
Final Energy/Atom
-3.9557 eV
Corrected Energy
-47.4681 eV
-47.4681 eV = -47.4681 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 262675
  • 15706
Submitted by
User remarks:
  • Barium dibromide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)