Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.213 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.298 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMo2C + C |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 288.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 172.9 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 33.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 27.2 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 19.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 54.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 244.5 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 298.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 172.9 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 33.3 |
SiC (mp-11714) | <0 0 1> | <1 1 1> | 33.3 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 249.8 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 54.3 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 54.3 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 38.4 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 38.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 38.4 |
ZrO2 (mp-2858) | <1 1 0> | <1 1 1> | 199.7 |
SiC (mp-7631) | <1 0 1> | <1 1 0> | 190.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 190.2 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 54.3 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 38.4 |
CaCO3 (mp-3953) | <1 0 1> | <1 1 0> | 271.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 298.9 |
CaCO3 (mp-3953) | <1 1 1> | <1 0 0> | 153.7 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 0> | 326.6 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 153.7 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 96.1 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 54.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 38.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 134.5 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 57.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 153.7 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 166.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 33.3 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 249.8 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 1> | 232.9 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 190.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 244.5 |
Ge (mp-32) | <1 1 1> | <1 1 1> | 232.9 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 81.5 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 190.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 217.4 |
GaTe (mp-542812) | <1 0 0> | <1 1 1> | 133.1 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 244.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 153.7 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 190.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 163.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 217.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
643 | 181 | 181 | 0 | 0 | 0 |
181 | 643 | 181 | 0 | 0 | 0 |
181 | 181 | 643 | 0 | 0 | 0 |
0 | 0 | 0 | 104 | 0 | 0 |
0 | 0 | 0 | 0 | 104 | 0 |
0 | 0 | 0 | 0 | 0 | 104 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
1.8 | -0.4 | -0.4 | -0.0 | -0.0 | 0.0 |
-0.4 | 1.8 | -0.4 | 0.0 | -0.0 | -0.0 |
-0.4 | -0.4 | 1.8 | 0.0 | 0.0 | 0.0 |
-0.0 | 0.0 | 0.0 | 9.6 | 0.0 | -0.0 |
-0.0 | -0.0 | 0.0 | 0.0 | 9.6 | -0.0 |
0.0 | -0.0 | 0.0 | -0.0 | -0.0 | 9.6 |
Shear Modulus GV155 GPa |
Bulk Modulus KV335 GPa |
Shear Modulus GR133 GPa |
Bulk Modulus KR335 GPa |
Shear Modulus GVRH144 GPa |
Bulk Modulus KVRH335 GPa |
Elastic Anisotropy0.81 |
Poisson's Ratio0.31 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.037 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
AgBr (mp-23231) | 0.0000 | 0.037 | 2 |
LiBr (mp-23259) | 0.0000 | 0.025 | 2 |
CeSb (mp-387) | 0.0000 | 0.000 | 2 |
EuSe (mp-21009) | 0.0000 | 0.000 | 2 |
UAs (mp-2104) | 0.0000 | 0.000 | 2 |
As (mp-10) | 0.0000 | 0.112 | 1 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.400 | 1 |
C (mp-998866) | 0.0000 | 2.755 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv C |
Final Energy/Atom-9.8232 eV |
Corrected Energy-19.6463 eV
-19.6463 eV = -19.6463 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)