Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-1.018 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.057 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Nb3S5 + NbP + P
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.020 125.1
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.020 212.4
MgO (mp-1265) <1 1 1> <0 1 0> 0.027 125.1
Al (mp-134) <1 0 0> <0 1 0> 0.034 291.8
CdS (mp-672) <1 1 0> <0 1 0> 0.057 250.1
Al2O3 (mp-1143) <1 0 1> <0 1 0> 0.065 333.5
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.071 147.1
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.078 208.4
NaCl (mp-22862) <1 1 1> <0 1 0> 0.079 166.8
BN (mp-984) <1 0 0> <0 0 1> 0.080 326.8
TiO2 (mp-390) <1 1 1> <0 1 1> 0.090 268.7
LiNbO3 (mp-3731) <0 0 1> <0 1 0> 0.094 166.8
GaN (mp-804) <1 0 0> <0 1 1> 0.099 134.3
SiC (mp-11714) <1 1 0> <0 1 1> 0.113 268.7
AlN (mp-661) <1 0 0> <1 1 1> 0.118 217.8
Fe3O4 (mp-19306) <1 1 0> <0 1 0> 0.119 208.4
TiO2 (mp-390) <1 0 1> <0 0 1> 0.133 196.1
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.144 245.1
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.157 261.5
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.158 70.7
DyScO3 (mp-31120) <0 1 1> <0 0 1> 0.161 212.4
Mg (mp-153) <0 0 1> <0 0 1> 0.166 114.4
InSb (mp-20012) <1 1 1> <1 0 0> 0.170 228.5
CdTe (mp-406) <1 1 1> <1 0 0> 0.173 228.5
TiO2 (mp-390) <1 1 0> <0 0 1> 0.177 212.4
SiC (mp-11714) <1 0 1> <0 1 1> 0.179 223.9
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.181 145.2
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.182 114.4
WS2 (mp-224) <0 0 1> <0 0 1> 0.182 114.4
GaN (mp-804) <1 1 1> <0 0 1> 0.204 212.4
LiTaO3 (mp-3666) <0 0 1> <0 1 0> 0.206 166.8
Au (mp-81) <1 1 0> <0 1 0> 0.209 125.1
Ni (mp-23) <1 1 0> <0 1 0> 0.223 208.4
ZrO2 (mp-2858) <1 0 -1> <0 1 1> 0.231 179.1
PbS (mp-21276) <1 1 1> <0 0 1> 0.231 310.5
LiF (mp-1138) <1 1 1> <0 0 1> 0.237 261.5
AlN (mp-661) <1 0 1> <0 0 1> 0.238 163.4
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.238 141.5
GaSe (mp-1943) <0 0 1> <0 1 0> 0.264 166.8
C (mp-48) <1 1 1> <0 0 1> 0.271 343.2
WS2 (mp-224) <1 0 1> <0 0 1> 0.288 228.8
YAlO3 (mp-3792) <0 1 1> <0 1 0> 0.290 291.8
Mg (mp-153) <1 0 0> <0 1 1> 0.297 134.3
Te2W (mp-22693) <0 1 1> <0 0 1> 0.298 114.4
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.311 196.1
Ni (mp-23) <1 0 0> <0 0 1> 0.313 49.0
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.313 212.4
CsI (mp-614603) <1 0 0> <0 0 1> 0.315 245.1
CdTe (mp-406) <1 0 0> <0 0 1> 0.317 130.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.324 130.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
313 84 67 0 0 0
84 254 109 0 0 0
67 109 170 0 0 0
0 0 0 97 0 0
0 0 0 0 72 0
0 0 0 0 0 57
Compliance Tensor Sij (10-12Pa-1)
3.6 -0.8 -0.9 0 0 0
-0.8 5.6 -3.3 0 0 0
-0.9 -3.3 8.4 0 0 0
0 0 0 10.4 0 0
0 0 0 0 13.8 0
0 0 0 0 0 17.4
Shear Modulus GV
77 GPa
Bulk Modulus KV
140 GPa
Shear Modulus GR
70 GPa
Bulk Modulus KR
132 GPa
Shear Modulus GVRH
73 GPa
Bulk Modulus KVRH
136 GPa
Elastic Anisotropy
0.58
Poisson's Ratio
0.27

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
144
U Values
--
Pseudopotentials
VASP PAW: P S Nb_pv
Final Energy/Atom
-7.3463 eV
Corrected Energy
-45.4045 eV
-45.4045 eV = -44.0775 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 16075

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)