Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.530 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP2S5 + Ag3PS4 |
Band Gap1.648 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 1 0> | <0 0 1> | 145.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 291.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 291.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 218.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 145.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 218.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 220.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 220.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 218.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 218.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 218.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 218.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 218.7 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 174.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 218.7 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 113.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 218.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 218.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 218.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 220.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 72.9 |
TeO2 (mp-2125) | <1 0 1> | <1 0 -1> | 227.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 218.7 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 218.7 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 218.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 291.6 |
C (mp-48) | <0 0 1> | <1 0 1> | 147.9 |
SiC (mp-11714) | <1 0 1> | <1 0 -1> | 227.8 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 218.7 |
C (mp-48) | <1 0 0> | <0 1 0> | 174.0 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 218.7 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 174.0 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 145.8 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 174.0 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 291.6 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 218.7 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 218.7 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 218.7 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 -1> | 227.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2P2PbO7 (mp-555933) | 0.6981 | 0.000 | 4 |
Li2Si2NiO6 (mp-767313) | 0.6948 | 0.092 | 4 |
LiCuPO4 (mp-757209) | 0.7269 | 0.089 | 4 |
Li2MnP2O7 (mp-761567) | 0.7244 | 0.062 | 4 |
Li2VP2O7 (mp-767710) | 0.7390 | 0.097 | 4 |
Ag7P3S11 (mp-683910) | 0.5286 | 0.013 | 3 |
K3UF3 (mp-675943) | 0.7308 | 0.503 | 3 |
Cu3P15I2 (mp-679930) | 0.6068 | 0.000 | 3 |
Cd3AsI3 (mp-676464) | 0.6632 | 0.000 | 3 |
Li2Ta2O3 (mp-675379) | 0.7329 | 0.530 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points34 |
U Values-- |
PseudopotentialsVASP PAW: P S Ag |
Final Energy/Atom-4.0988 eV |
Corrected Energy-115.8567 eV
-115.8567 eV = -106.5683 eV (uncorrected energy) - 9.2884 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)