@article{Mucker1968, author = "Mucker, K.D.S. and Smith, G.S. and Johnson, Q.", title = "The crystal structure of Re Cl5", journal = "Acta Crystallographica B (24,1968-38,1982)", year = "1968", volume = "24", pages = "874-879", ASTM_id = "ACBCAR" }