Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.124 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 312.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 300.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 312.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 265.2 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 265.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 293.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 312.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 176.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 97.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 312.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 300.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 312.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 300.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 62.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 293.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 250.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 312.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 150.1 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 265.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 187.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 88.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 300.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 195.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 250.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 225.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 312.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 300.1 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 265.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 75.0 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 293.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 312.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 312.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 293.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 225.1 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 293.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 312.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 312.6 |
LaF3 (mp-905) | <0 0 1> | <1 1 0> | 88.4 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 265.2 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 88.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 75.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 312.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 150.1 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 293.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 312.6 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 312.6 |
Ni (mp-23) | <1 1 1> | <1 0 1> | 293.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 75.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
101 | 16 | 16 | 0 | 0 | 0 |
16 | 89 | 31 | 0 | 0 | 0 |
16 | 31 | 89 | 0 | 0 | 0 |
0 | 0 | 0 | 36 | 0 | 0 |
0 | 0 | 0 | 0 | 31 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.4 | -1.4 | -1.4 | 0 | 0 | 0 |
-1.4 | 13 | -4.3 | 0 | 0 | 0 |
-1.4 | -4.3 | 13 | 0 | 0 | 0 |
0 | 0 | 0 | 27.9 | 0 | 0 |
0 | 0 | 0 | 0 | 32.6 | 0 |
0 | 0 | 0 | 0 | 0 | 32.6 |
Shear Modulus GV34 GPa |
Bulk Modulus KV45 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR45 GPa |
Shear Modulus GVRH33 GPa |
Bulk Modulus KVRH45 GPa |
Elastic Anisotropy0.10 |
Poisson's Ratio0.20 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoCoSn (mp-5601) | 0.6777 | 0.000 | 3 |
DyCoSn (mp-22228) | 0.6570 | 0.000 | 3 |
TbCoSn (mp-646450) | 0.6751 | 0.000 | 3 |
ErCoSn (mp-11851) | 0.6786 | 0.000 | 3 |
GdGeRu (mp-19714) | 0.6803 | 0.000 | 3 |
PbCl2 (mp-619071) | 0.6267 | 0.023 | 2 |
MgSi2 (mp-1073529) | 0.6391 | 0.205 | 2 |
MgSi2 (mp-1073469) | 0.6119 | 0.252 | 2 |
MgSi2 (mp-1073663) | 0.6219 | 0.233 | 2 |
Mg2Si (mp-1074751) | 0.6394 | 0.185 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ga_d |
Final Energy/Atom-2.7444 eV |
Corrected Energy-38.4223 eV
-38.4223 eV = -38.4223 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)