Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.836 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa20As13 + Ba |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 339.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.2 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 266.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 191.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 313.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 234.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 130.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 208.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 276.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 276.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 208.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 130.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 286.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 260.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 130.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 191.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 286.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 266.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 208.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 276.7 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 276.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 130.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 339.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 276.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 130.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 130.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 78.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 286.9 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 260.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 208.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 130.4 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 234.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 130.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 365.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 208.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 339.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 208.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 156.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 52.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 313.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 208.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 191.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 208.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 104.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 286.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 130.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 130.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 276.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 234.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 365.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
42 | 7 | 15 | 0 | 0 | 0 |
7 | 42 | 15 | 0 | 0 | 0 |
15 | 15 | 69 | 0 | 0 | 0 |
0 | 0 | 0 | 10 | 0 | 0 |
0 | 0 | 0 | 0 | 10 | 0 |
0 | 0 | 0 | 0 | 0 | 17 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
26.1 | -2.8 | -5 | 0 | 0 | 0 |
-2.8 | 26.1 | -5 | 0 | 0 | 0 |
-5 | -5 | 16.7 | 0 | 0 | 0 |
0 | 0 | 0 | 100.7 | 0 | 0 |
0 | 0 | 0 | 0 | 100.7 | 0 |
0 | 0 | 0 | 0 | 0 | 57.5 |
Shear Modulus GV15 GPa |
Bulk Modulus KV25 GPa |
Shear Modulus GR14 GPa |
Bulk Modulus KR23 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH24 GPa |
Elastic Anisotropy0.67 |
Poisson's Ratio0.25 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
USiS (mp-7932) | 0.2978 | 0.579 | 3 |
NiGePd (mp-3274) | 0.3756 | 0.000 | 3 |
TbTiGe (mp-10078) | 0.4064 | 0.022 | 3 |
TbScGe (mp-4395) | 0.3894 | 0.005 | 3 |
NiAsRh (mp-19768) | 0.3314 | 0.000 | 3 |
Ba2Sb (mp-9908) | 0.1877 | 0.016 | 2 |
Ba2Bi (mp-567872) | 0.2030 | 0.025 | 2 |
EuO2 (mp-1018700) | 0.1866 | 0.149 | 2 |
Ca2As (mp-10106) | 0.2051 | 0.041 | 2 |
Sr2As (mp-15697) | 0.1286 | 0.075 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv As |
Final Energy/Atom-3.6684 eV |
Corrected Energy-22.0105 eV
-22.0105 eV = -22.0105 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)