Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.159 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.656 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/acd [142] |
HallI 4bw 2aw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiGa2O5 (mp-760501) | 0.6686 | 0.039 | 3 |
Hf3N2O3 (mp-760360) | 0.6806 | 0.071 | 3 |
LiMnF3 (mp-763191) | 0.6703 | 0.103 | 3 |
Zr3N2O3 (mp-754659) | 0.6794 | 0.062 | 3 |
TiAl2O5 (mp-4930) | 0.6822 | 0.013 | 3 |
LiMnOF2 (mp-763872) | 0.7133 | 0.108 | 4 |
LiCo2O2F3 (mp-850987) | 0.7174 | 0.303 | 4 |
Nb2Zn2SbO8 (mvc-3) | 0.7341 | 0.134 | 4 |
Ti3O5 (mp-8057) | 0.7422 | 0.014 | 2 |
Ti3O5 (mp-556480) | 0.7471 | 0.009 | 2 |
LiP5 (mp-2412) | 0.7481 | 0.014 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv P |
Final Energy/Atom-5.1342 eV |
Corrected Energy-328.5895 eV
-328.5895 eV = -328.5895 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)