Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.573 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.427 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 201.2 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 94.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 213.0 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 277.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 255.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 159.8 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 282.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 127.7 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 188.2 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 134.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 199.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 213.0 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 249.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 255.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 268.3 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 249.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 266.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 282.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 191.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 213.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 249.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 207.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 319.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 276.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 268.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 249.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 191.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 319.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 213.0 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 127.7 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 255.5 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 319.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 255.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 319.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 99.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 201.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 213.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 213.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 201.2 |
C (mp-66) | <1 1 0> | <1 0 1> | 199.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 266.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 319.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 276.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 134.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 69.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 255.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 213.0 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 319.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.00 | -0.00 | -0.28 |
-0.00 | 2.31 | 0.00 |
-0.28 | 0.00 | 2.68 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.53 | -0.00 | -5.23 |
-0.00 | 4.75 | 0.00 |
-5.23 | 0.00 | 15.44 |
Polycrystalline dielectric constant
εpoly∞
2.66
|
Polycrystalline dielectric constant
εpoly
8.91
|
Refractive Index n1.63 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H7IN2 (mp-721084) | 0.6814 | 0.000 | 3 |
PAuCl4 (mp-23355) | 0.5525 | 0.000 | 3 |
Co(CO)4 (mp-543072) | 0.4895 | 0.527 | 3 |
H12C5N2O (mp-554659) | 0.4598 | 0.156 | 4 |
H13C4NF2 (mp-554840) | 0.4559 | 0.122 | 4 |
CsCo(CO)4 (mp-540895) | 0.5351 | 0.322 | 4 |
K3Cu(CN)4 (mp-6610) | 0.5397 | 0.057 | 4 |
BN(OF2)2 (mp-555207) | 0.3578 | 0.000 | 4 |
C5N4 (mp-651723) | 0.5373 | 0.554 | 2 |
CrO3 (mp-779986) | 0.7068 | 0.096 | 2 |
Tc2O7 (mp-27485) | 0.3810 | 0.000 | 2 |
FeBN3O3F4 (mp-631397) | 0.6890 | 0.417 | 5 |
BH5CSN2 (mp-706606) | 0.7256 | 0.234 | 5 |
H3AuC2NCl (mp-569084) | 0.6240 | 0.286 | 5 |
BH11AuC4IN2 (mp-698289) | 0.6438 | 0.231 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: N Cl O |
Final Energy/Atom-4.9077 eV |
Corrected Energy-86.7675 eV
Uncorrected energy = -78.5235 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -86.7675 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)